Effects of temperature and normal load on tribological behavior of nickel-based high temperature self-lubricating wear-resistant composite coating

NiCr/Cr3C2–WS2–CaF2 mixed powders were designed and aimed to fabricate high temperature self-lubricating wear-resistant composite coating by laser cladding. The friction and wear properties of the coating were investigated under different temperatures and loads against Si3N4 ceramic ball. Results show that friction coefficient decreases with the increasing temperature while the wear rate firstly decreases and then increases with the increasing temperature. Both the friction coefficient and wear rate firstly decreases and then slightly increases with the increasing normal load. The coating exhibits relatively excellent tribological behavior under moderate temperature and moderate normal load.

[1]  Xiulin Liu,et al.  Microstructure and dry sliding wear behavior of Fe2TiSi /γ-Fe/Ti5Si3 composite coating fabricated by plasma transferred arc cladding process , 2010 .

[2]  Xianglin Zhang,et al.  Microstructure and properties of HVOF sprayed Ni-based submicron WS2/CaF2 self-lubricating composite coating , 2009 .

[3]  R. Tenne,et al.  Tribological properties of WS2 nanoparticles under mixed lubrication , 2003 .

[4]  J. Zabinski,et al.  Sulfate based coatings for use as high temperature lubricants , 1999 .

[5]  Hua-ming Wang,et al.  Microstructure and tribological properties of laser clad CaF2/Al2O3 self-lubrication wear-resistant ceramic matrix composite coatings , 2002 .

[6]  Fujie Li,et al.  Laser cladding of stainless steel with Ni–Cr3C2 for improved wear performance , 2001 .

[7]  Xiubo Liu,et al.  Microstructure and wear behaviors of laser clad NiCr/Cr3C2–WS2 high temperature self-lubricating wear-resistant composite coating , 2012 .

[8]  D. Xiong,et al.  Effect of load and sliding speed on friction and wear behavior of silver/h-BN containing Ni-base P/M composites , 2011 .

[9]  Xiong Dangsheng Lubrication behavior of Ni–Cr-based alloys containing MoS2 at high temperature , 2001 .

[10]  S. Sasaki,et al.  Microstructure and tribological properties of ZrO2(Y2O3) matrix composites doped with different solid lubricants from room temperature to 800 °C , 2009 .

[11]  Hua-ming Wang,et al.  Microstructure and dry sliding wear resistance of laser clad TiC reinforced Ti–Ni–Si intermetallic composite coating , 2009 .

[12]  Wen-jie Ma,et al.  Effect of surface texture on transfer layer formation and tribological behaviour of copper-graphite composite , 2011 .

[13]  Wei-min Liu,et al.  A study of Ni3Si-based composite coating fabricated by self-propagating high temperature synthesis casting route , 2011 .

[14]  W. Zhang,et al.  Preparation and characterization of atmospheric plasma-sprayed NiCr/Cr3C2–BaF2·CaF2 composite coating , 2009 .

[15]  R. Yu,et al.  Influences of precursor constitution and processing speed on microstructure and wear behavior during laser clad composite coatings on γ-TiAl intermetallic alloy , 2009 .

[16]  A. Erdemir,et al.  Solid Lubricant Coatings: Recent Developments and Future Trends , 2004 .

[17]  Jiansong Zhou,et al.  Friction and wear behavior of laser cladding Ni/hBN self-lubricating composite coating , 2008 .

[18]  Hua-ming Wang,et al.  Microstructure and tribological properties of laser clad γ/Cr7C3/TiC composite coatings on γ-TiAl intermetallic alloy , 2007 .

[19]  D. Xiong,et al.  Elevated temperature tribological behavior of Ni based composites containing nano-silver and hBN , 2010 .

[20]  Christopher DellaCorte,et al.  The effect of counterface on the tribological performance of a high temperature solid lubricant composite from 25 to 650°C , 1996 .

[21]  Hua-ming Wang,et al.  Metallic tribological compatibility of laser clad Mo2Ni3Si/NiSi metal silicide coatings , 2005 .

[22]  J. Hao,et al.  Tribological properties of solid lubricants (graphite, h-BN) for Cu-based P/M friction composites , 2008 .

[23]  S. R. Bakshi,et al.  Microstructure and wear properties of aluminum/aluminum–silicon composite coatings prepared by cold spraying , 2009 .

[24]  Sinésio Domingues Franco,et al.  Effect of temperature, normal load and pre-oxidation on the sliding wear of multi-component ferrous alloys , 2005 .

[25]  C. Xie,et al.  Ni-based alloy/submicron WS2 self-lubricating composite coating synthesized by Nd:YAG laser cladding , 2008 .

[26]  S. Shi,et al.  Microstructure and wear behavior of γ/Al4C3/TiC/CaF2 composite coating on γ-TiAl intermetallic alloy prepared by Nd:YAG laser cladding , 2009 .

[27]  Mao Yang,et al.  Elevated temperature dry sliding wear behavior of nickel-based composite coating on austenitic stainless steel deposited by a novel central hollow laser cladding , 2011 .

[28]  Jiansong Zhou,et al.  Preparation, microstructure and tribological properties of Ni3Al intermetallic compound coating by laser cladding , 2010 .

[29]  Weigang Zhang,et al.  Effects of solid lubricant content on the microstructure and properties of NiCr/Cr3C2–BaF2·CaF2 composite coatings , 2009 .