Effect of luting composite shrinkage and thermal loads on the stress distribution in porcelain laminate veneers.

STATEMENT OF PROBLEM Cyclic thermal fatigue has demonstrated a significant influence of the thicknesses of luting composite and ceramic in crack propensity of porcelain laminates. PURPOSE This study was conducted to define potentially involved parameters for crack development in porcelain laminates bonded to teeth. Finite element modeling was used to evaluate the respective effects of luting composite shrinkage and significant thermal changes. MATERIAL AND METHODS A buccolingual cross-section of a maxillary incisor was digitized and used as a template to generate a single 2-dimensional mesh, including all the different restorative designs. Luting composite shrinkage was simulated at a baseline temperature of 20 degrees C. The effect of thermal loads from 20 degrees C to 5 degrees C and from 20 degrees C to 50 degrees C was assessed with and without preexisting composite shrinkage. RESULTS Shrinkage of the luting composite alone generated important compressive forces on the ceramic, either at the restoration surface or interface. Compression intensity was related to geometry and ratio of thicknesses between the ceramic and luting composite (CER/CPR). Lower ratios produced higher compression forces in the ceramic. When thermal loads were combined to the composite shrinking forces, the stress pattern was significantly changed only for the experimental conditions with the lowest CER/CPR ratio. Temperature increase reduced compressive stresses and exacerbated tensile stresses. Thermal loads were simulated alone (situation of an "ideal nonshrinking" luting composite) and generated mainly tensile stresses in the ceramic, which intensity was again modulated by the CER/CPR ratio and the local geometry of composite and ceramic. Because of ceramic brittleness, these tensile forces were more detrimental than the high compression created by composite shrinkage alone. The stress pattern was not influenced by the incisal length of the veneer but rather by the facial thickness of ceramic. The worst record made with a shrinking luting agent (500 microm of luting composite, lowest CER/CPR ratio, 5 degrees C) was much less harmful than the worst record made with a hypothetical "nonshrinking" luting material. CONCLUSIONS The ratio of the thickness of cement and luting composite appears to have a relevant influence on the stress distribution in porcelain laminates. Restorations that are too thin, combined with poor internal fit, resulted in higher stresses at both the surface and interface of the restoration. Because of its precompressed state given by composite shrinkage, ceramics performed better with regard to temperature-induced tensile forces.

[1]  D. Watts,et al.  Temperature-dependence of Compressive Properties of Human Dentin , 1987, Journal of dental research.

[2]  R. Bowen,et al.  Adhesive bonding of various materials to hard tooth tissues: forces developing in composite materials during hardening. , 1983, Journal of the American Dental Association.

[3]  M. MacEntee,et al.  Porcelain and resin veneers clinically evaluated: 2-year results. , 1990, Journal of the American Dental Association.

[4]  T. Wang,et al.  Measurement of thermal expansion coefficient of human teeth. , 1990, Australian dental journal.

[5]  R. G. Craig Restorative dental materials , 1971 .

[6]  Wang Tong,et al.  Measurement of thermal expansion coefficient of human teeth , 1989 .

[7]  U. Belser,et al.  Natural and restorative oral esthetics. Part II: Esthetic treatment modalities. , 1993, Journal of esthetic dentistry.

[8]  T W Korioth,et al.  Modeling the mechanical behavior of the jaws and their related structures by finite element (FE) analysis. , 1997, Critical reviews in oral biology and medicine : an official publication of the American Association of Oral Biologists.

[9]  A. Plasschaert,et al.  Failure Stress Criteria for Composite Resin , 1987, Journal of dental research.

[10]  M. Barco,et al.  Temperature extremes produced orally by hot and cold liquids. , 1992, The Journal of prosthetic dentistry.

[11]  P Magne,et al.  Ceramic laminate veneers: continuous evolution of indications. , 1997, Journal of esthetic dentistry.

[12]  R DeLong,et al.  Biophysical stress analysis of restored teeth: modelling and analysis. , 1988, Dental materials : official publication of the Academy of Dental Materials.

[13]  P. Magne,et al.  An in vitro study of parameters related to marginal and internal seal of bonded restorations. , 1993, Quintessence international.

[14]  L. Watanabe,et al.  In vitro microleakage at the gingival margin of porcelain and resin veneers. , 1992, The Journal of prosthetic dentistry.

[15]  A. Versluis,et al.  Thermal expansion coefficient of dental composites measured with strain gauges. , 1996, Dental materials : official publication of the Academy of Dental Materials.

[16]  T. Berry,et al.  Post-bonding crack formation in porcelain veneers. , 1997, Journal of esthetic dentistry.

[17]  R. Jacobi,et al.  The ceramic reverse three-quarter crown for anterior teeth: preparation design. , 1989, The Journal of prosthetic dentistry.

[18]  R DeLong,et al.  Biophysical stress analysis of restored teeth: experimental strain measurement. , 1988, Dental materials : official publication of the Academy of Dental Materials.

[19]  J. Hodges,et al.  Crack propensity of porcelain laminate veneers: A simulated operatory evaluation. , 1999, The Journal of prosthetic dentistry.

[20]  E. Munksgaard,et al.  Treatment of crown fractured incisors with laminate veneer restorations. An experimental study. , 1992, Endodontics & dental traumatology.

[21]  C. Fairhurst,et al.  Bond strength and mechanical properties of dental porcelain enamels. , 1967, The Journal of prosthetic dentistry.

[22]  A. Caputo,et al.  A photoelastic study of stresses on porcelain laminate preparations. , 1987, The Journal of prosthetic dentistry.

[23]  C. Davidson,et al.  Relaxation of Polymerization Contraction Stresses by Flow in Dental Composites , 1984, Journal of dental research.

[24]  J. Calamia Clinical evaluation of etched porcelain veneers. , 1989, American journal of dentistry.

[25]  K J Anusavice,et al.  Influence of Incisal Length of Ceramic and Loading Orientation on Stress Distribution in Ceramic Crowns , 1988, Journal of dental research.

[26]  J. Hood,et al.  Impact fracture characteristics of intact and crowned human central incisors. , 1993, Journal of oral rehabilitation.

[27]  W. Johnston,et al.  Incisal-edge strength of porcelain laminate veneers restoring mandibular incisors. , 1992, The International journal of prosthodontics.