Performance and Aging of a 20-Year-Old Silicon PV System

This paper examines the long-term performance of a 20-year-old crystalline silicon system. The degradation was found to be about 0.8%/year and is consistent with historical averages. In contrast with the majority of historical degradation, the decline for this particular system is more attributable to fill factor (FF) than to short-circuit current (Isc). The underlying cause was determined to be an increase in series resistance. We found no evidence that this system degrades significantly differently from its worst performing strings and modules. Maintenance events during the 20 years were dominated by inverter issues with a total of four replacements.

[1]  Steven S. Hegedus,et al.  Thin‐film solar cells: device measurements and analysis , 2004 .

[2]  S. Rummel,et al.  PV cell and module performance measurement capabilities at NREL , 1998 .

[3]  S. Kurtz,et al.  Analytical improvements in PV degradation rate determination , 2010, 2010 35th IEEE Photovoltaic Specialists Conference.

[4]  Dirk C. Jordan,et al.  The Dark Horse of Evaluating Long-Term Field Performance—Data Filtering , 2014, IEEE Journal of Photovoltaics.

[5]  S. Sakamoto,et al.  Field test results on the stability of crystalline silicon photovoltaic modules manufactured in the 1990s , 2003, 3rd World Conference onPhotovoltaic Energy Conversion, 2003. Proceedings of.

[6]  B. Marion,et al.  Long-Term Performance of the SERF PV Systems , 2003 .

[7]  Dirk C. Jordan,et al.  Technology and Climate Trends in PV Module Degradation: Preprint , 2012 .

[8]  A. Golnas,et al.  PV system reliability: An operator's perspective , 2013, 2012 IEEE 38th Photovoltaic Specialists Conference (PVSC) PART 2.

[9]  D. L. King,et al.  Commonly observed degradation in field-aged photovoltaic modules , 2002, Conference Record of the Twenty-Ninth IEEE Photovoltaic Specialists Conference, 2002..

[10]  Dirk C. Jordan,et al.  Photovoltaic Degradation Rates—an Analytical Review , 2012 .

[11]  M. Green Solar Cells : Operating Principles, Technology and System Applications , 1981 .

[12]  F. Chenlo,et al.  Early degradation of silicon PV modules and guaranty conditions , 2011 .

[13]  E. Kaplani Detection of Degradation Effects in Field-Aged c-Si Solar Cells through IR Thermography and Digital Image Processing , 2012 .

[14]  Sarah Kurtz,et al.  Photovoltaic Module Qualification Plus Testing , 2014, 2014 IEEE 40th Photovoltaic Specialist Conference (PVSC).