Since a laptop caught fire in 2006 at the latest, Li-ion cells were considered as more dangerous than other accumulators [1]. Recent incidents, such as the one involving a BYD e6 electric taxi [2] or the Boeing Dreamliner [3], give rise to questions concerning the safety of L#i-ion cells. This is a crucial point, since Li-ion cells are increasingly integrated in all kinds of (electric) vehicles. Therefore the economic success of hybrid electric vehicles (HEV) and battery electric vehicles (BEV) depends significantly on the safety of Li-ion cells. Lithium nickel manganese cobalt oxide (NMC) and lithium nickel cobalt aluminium oxide (NCA) are two standard Li-ion cathode chemistries, which are often used for today’s HEVs and BEVs Li-ion batteries. Cells with this two cathode technologies are investigated in detail and compared to cells with the alleged save lithium iron phosphate (LFP) technology. Furthermore only commercially available and mass produced Li-ion cells were tested, in order to get as close to real end-user applications as possible. To ensure comparability, cells with the most common 18650 casing have been used. Furthermore all cells had no built-in resistor with positive temperature coefficient (PTC-device). For each abuse test at least 2 cells have been tested to get to know the statistical dispersion. The spread was in all tests for all measured values of each cell type lower than 11 %. Consequently it can be supposed, that mass produced cells show equal behaviour also in abusive test. The performed electrical safety tests on these cells, involve overcharge, overdischarge and short circuit tests. These tests represent real abuse scenarios and are geared to established standards [15], [16], [17], [18]. To complete these measurements an accelerated rate calorimetry (ARC) test has been carried out, to determine the thermal stability of the cells. As in the literature discussed, the investigated LFP/C cells show a higher thermal stability and are therefore safer, although they do not have any overcharge buffer as the investigated NCA/C and NMC/C cells.
[1]
M. Behm,et al.
Investigation of Short-Circuit Scenarios in a Lithium-Ion Battery Cell
,
2012
.
[2]
H. Maleki,et al.
Effects of overdischarge on performance and thermal stability of a Li-ion cell
,
2006
.
[3]
Michel Perrier,et al.
LiFePO4 safe Li-ion polymer batteries for clean environment
,
2005
.
[4]
Yuichi Sato,et al.
Overcharge reaction of lithium-ion batteries
,
2005
.
[5]
Hiroaki Ishikawa,et al.
Study of thermal deterioration of lithium-ion secondary cell using an accelerated rate calorimeter (ARC) and AC impedance method
,
2012
.
[6]
J. Yamaki,et al.
Lithium Ion Cell Safety
,
2000
.
[7]
J. Dahn,et al.
Accelerating Rate Calorimetry Study on the Thermal Stability of Lithium Intercalated Graphite in Electrolyte. I. Experimental
,
1999
.
[8]
Shaopeng Zhang,et al.
Effect of Overdischarge on Swelling and Recharge Performance of Lithium Ion Cells
,
2008
.
[9]
Junwei Jiang,et al.
ARC studies of the thermal stability of three different cathode materials: LiCoO2; Li[Ni0.1Co0.8Mn0.1]O2; and LiFePO4, in LiPF6 and LiBoB EC/DEC electrolytes
,
2004
.
[10]
Dmitry Belov,et al.
Failure mechanism of Li-ion battery at overcharge conditions
,
2008
.
[11]
K. S. Nanjundaswamy,et al.
Phospho‐olivines as Positive‐Electrode Materials for Rechargeable Lithium Batteries
,
1997
.
[12]
Daniel H. Doughty,et al.
A General Discussion of Li Ion Battery Safety
,
2012
.
[13]
R. Spotnitz,et al.
Abuse behavior of high-power, lithium-ion cells
,
2003
.
[14]
E. Roth,et al.
Thermal abuse performance of high-power 18650 Li-ion cells
,
2004
.