Nanoporous gold by dealloying of an amorphous precursor
暂无分享,去创建一个
[1] L. Battezzati,et al. De-alloying kinetics of an Au-based amorphous alloys , 2012 .
[2] A. Schaefer,et al. Toward Controlled Modification of Nanoporous Gold. A Detailed Surface Science Study on Cleaning and Oxidation , 2012 .
[3] Xiaoping Song,et al. Nanoporous Ag prepared from the melt-spun Cu-Ag alloys , 2011 .
[4] J. Erlebacher,et al. Mechanism of coarsening and bubble formation in high-genus nanoporous metals. , 2011, Physical review letters.
[5] D. Allara,et al. Nanoporous Gold: A High Sensitivity and Specificity Biosensing Substrate , 2011 .
[6] J. Weissmüller,et al. Bulk Nanoporous Metal for Actuation , 2010 .
[7] Z. Qi,et al. Formation of ultrafine nanoporous gold related to surface diffusion of gold adatoms during dealloying of Al2Au in an alkaline solution , 2010 .
[8] A. Inoue,et al. Novel Nanoporous Au-Pd Alloy with High Catalytic Activity and Excellent Electrochemical Stability , 2010 .
[9] J. Erlebacher,et al. Hard Materials with Tunable Porosity , 2009 .
[10] J. Erlebacher,et al. Relationship between the parting limit for de-alloying and a particular geometric high-density site percolation threshold , 2009 .
[11] B. Schmitt,et al. On the microstructure of nanoporous gold: an X-ray diffraction study. , 2008, Nano letters.
[12] Mingwei Chen,et al. Ultrafine nanoporous gold by low-temperature dealloying and kinetics of nanopore formation , 2007 .
[13] J. Galvele,et al. Stress corrosion cracking of 18 carat gold , 2004 .
[14] S. Corcoran,et al. Dealloying of Ag-Au Alloys in Halide-Containing Electrolytes Affect on Critical Potential and Pore Size , 2003 .
[15] J. Erlebacher,et al. The Dealloying Critical Potential , 2002 .
[16] A. Arvia,et al. Kinetics of Particle Coarsening at Gold Electrode/Electrolyte Solution Interfaces Followed by In Situ Scanning Tunneling Microscopy , 1996 .
[17] J. González-Velasco,et al. Mechanism of surface diffusion of gold adatoms in contact with an electrolytic solution , 1993 .
[18] A. Arvia,et al. Effect of the solution composition and the applied potential on the kinetics of roughness relaxation at gold electrodes in slightly acid electrolytes , 1993 .
[19] H. Pickering,et al. Stress corrosion cracking of Cu18%Au in 1N Na2SO4 - 0.01N H2SO4 , 1988 .
[20] K. Sieradzki,et al. Stress Corrosion Cracking , 2001 .
[21] H. Pickering. Characteristic features of alloy polarization curves , 1983 .
[22] P. J. Byrne,et al. On Preferential Anodic Dissolution of Alloys in the Low‐Current Region and the Nature of the Critical Potential , 1971 .