Influence de la temperature minimale du cycle de gel - degel sur la deterioration du beton par ecaillage en presence de sels fondants
暂无分享,去创建一个
Eight different concrete mixtures were prepared to investigate the influence of the minimum temperature of the freezing and thawing cycle on scaling deterioration due to deicer salt. In addition to the two minimum temperatures studied (−18 and −9 °C), test variables included the type of binder (with or without silica fume), the water/binder ratio (0.35 or 0.45), the characteristics of the air-void network (with or without air entrainment), and the drying temperature during the conditioning period prior to the scaling test (20, 40, or 110 °C). The scaling resistance to deicer salt of all concrete mixtures was assessed according to the prescriptions of the ASTM C672 test procedure using a 3 % NaCl solution. Test results indicate that a reduction of the minimal temperature from −9 to −18 °C significantly increases the scaling deterioration of concrete due to deicer salt. Key words: freezing cycle, scaling resistance, minimal freezing temperature, deicer salts.