Characterisation of electroplated Sn/Ag solder bumps

[1]  C. Lee,et al.  High density fine pitch Pb-free flip-chip interconnect assembly , 2003, Electronic Packaging Technology Conference.

[2]  Nduka Nnamdi (Ndy) Ekere,et al.  Establishing control factors of intermetallic formation mithin Pb-free solder bumps at flip chip gometries , 2003, 53rd Electronic Components and Technology Conference, 2003. Proceedings..

[3]  K. Feldmann,et al.  Lead-free low-cost flip-chip process chain: layout, process, reliability , 2002, 27th Annual IEEE/SEMI International Electronics Manufacturing Technology Symposium.

[4]  T. Ritzdorf,et al.  Electrodeposition of ternary near-eutectic SnAgCu solders with an alkaline bath , 2002, 2002 Proceedings. 8th International Advanced Packaging Materials Symposium (Cat. No.02TH8617).

[5]  R. Kiumi,et al.  Process development of electroplate bumping for ULSI flip chip technology , 2002, 52nd Electronic Components and Technology Conference 2002. (Cat. No.02CH37345).

[6]  G. Chou Microstructure evolution of SnPb and SnAg/Cu BGA solder joints during thermal aging , 2002, 2002 Proceedings. 8th International Advanced Packaging Materials Symposium (Cat. No.02TH8617).

[7]  H. Reichl,et al.  Pb-free Sn/3.5Ag electroplating bumping process and under bump metallization (UBM) , 2002 .

[8]  D. Frear,et al.  Pb-free solders for flip-chip interconnects , 2001 .

[9]  Jong-Kai Lin,et al.  Pb-free solder paste reflow window study for flip chip wafer bumping , 2001, Proceedings International Symposium on Advanced Packaging Materials Processes, Properties and Interfaces (IEEE Cat. No.01TH8562).

[10]  R. Schetty,et al.  Lead-free bump interconnections for flip-chip applications , 2000, Twenty Sixth IEEE/CPMT International Electronics Manufacturing Technology Symposium (Cat. No.00CH37146).

[11]  K. N. Subramanian,et al.  Formation and growth of interfacial intermetallic layers in eutectic Sn-Ag solder and its composite solder joints , 2000 .

[12]  J. Yoshioka,et al.  Eutectic Sn-Ag solder bump process for ULSI flip chip technology , 2000, 2000 Proceedings. 50th Electronic Components and Technology Conference (Cat. No.00CH37070).

[13]  Yi-Cheng Liu,et al.  Reflow and property of Al/Cu/electroless nickel/Sn-Pb solder bumps , 1999, ECTC 1999.

[14]  Tsung-Yu Pan,et al.  Intermetallic compound growth on Ni, Au/Ni, and Pd/Ni substrates with Sn/Pb, Sn/Ag, and Sn solders [PWBs] , 1998, 1998 Proceedings. 48th Electronic Components and Technology Conference (Cat. No.98CH36206).

[15]  W. Brown,et al.  Flip chip interconnects with electroplated, extended eutectic solder , 1998, Proceedings. 1998 International Conference on Multichip Modules and High Density Packaging (Cat. No.98EX154).

[16]  H. Steen,et al.  Development and validation of a lead-free alloy for solder paste applications , 1997 .

[17]  S. Jin,et al.  The design and properties of new, Pb-free solder alloys , 1994, Proceedings of 16th IEEE/CPMT International Electronic Manufacturing Technology Symposium.

[18]  D. Shangguan,et al.  Evaluation of lead-free eutectic Sn-Ag solder for automotive electronics packaging applications , 1994, Proceedings of 16th IEEE/CPMT International Electronic Manufacturing Technology Symposium.