Influence of FSP on the microstructure, microhardness, intergranular corrosion susceptibility and wear resistance of AA5083 alloy

ABSTRACT This article investigates the role of friction stir processing (FSP) process parameters on the evolution of microstructure, hardness, intergranular corrosion resistance and wear resistance of aluminium alloy AA5083. The FSP trials are performed by changing the process parameters as per face-centered central composite design. The friction stir processed (FSPed) specimens subjected to intergranular corrosion test and wear test are characterized using field emission scanning electron microscope, energy dispersive x-ray spectroscopy and X-ray diffraction. Outcomes suggest that grain refinement, dispersion and partial dissolution of secondary phase has simultaneously increased the hardness, intergranular corrosion resistance and wear resistance of the FSPed specimens. The study found that tool rotation speed of 700 rpm, tool traverse speed of 60 mm min−1 and shoulder diameter of 15 mm results in maximum hardness, wear resistance and intergranular corrosion resistance.

[1]  Vaira Vignesh Ramalingam,et al.  Modelling Corrosion Behavior of Friction Stir Processed Aluminium Alloy 5083 Using Polynomial: Radial Basis Function , 2017, Transactions of the Indian Institute of Metals.

[2]  S. Thirumalini,et al.  Numerical modelling of thermal phenomenon in friction stir welding of aluminum plates , 2016 .

[3]  V. Sharma,et al.  Friction Stir Processing Strategies for Uniform Distribution of Reinforcement in a Surface Composite , 2016 .

[4]  K. Karthick,et al.  Process parameters effect on the strength of Friction Stir Spot Welded AA6061 , 2016 .

[5]  Vipin,et al.  Fabrication of Al5083/B4C surface composite by friction stir processing and its tribological characterization , 2015 .

[6]  A. Riahi,et al.  The effect of surface conditions on the elevated temperature sliding contact deformation of AA5083 alloy , 2015 .

[7]  Pedro Vilaça,et al.  Surface reinforcement of AA5083-H111 by friction stir processing assisted by electrical current , 2015 .

[8]  A. Nagode,et al.  Superplasticity of the rolled and friction stir processed Al–4.5 Mg–0.35Sc–0.15Zr alloy , 2014 .

[9]  R. Mishra,et al.  Fundamental Physical Metallurgy Background for FSW/P , 2014 .

[10]  A. Riahi,et al.  The tribological behaviour of AA5083 alloy plastically deformed at warm forming temperatures , 2013 .

[11]  M. K. Besharati Givi,et al.  Mechanical Properties, Corrosion Resistance, and Microstructural Changes during Friction Stir Processing of 5083 Aluminum Rolled Plates , 2012 .

[12]  V. Ratna Kishore,et al.  Effect of Axial Pressure and Tool Rotation Speed on Temperature Distribution during Dissimilar Friction Stir Welding , 2011 .

[13]  G. Elsner,et al.  Aluminium and aluminium alloys , 2011 .

[14]  H. Spies Surface engineering of aluminium and titanium alloys: An overview , 2010 .

[15]  G. Cui,et al.  The origin of non-uniform microstructure and its effects on the mechanical properties of a friction stir processed Al–Mg alloy , 2009 .

[16]  Z. Ma,et al.  Friction Stir Processing Technology: A Review , 2008 .

[17]  C. Panagopoulos,et al.  Wear behaviour of 5083 wrought aluminium alloy under free corrosion conditions , 2007 .

[18]  R. Mishra,et al.  Enhanced superplasticity through friction stir processing in continuous cast AA5083 aluminum , 2007 .

[19]  M. Mahoney,et al.  The effect of friction stir processing on 5083-H321/5356 Al arc welds: Microstructural and mechanical analysis , 2006 .

[20]  M. D. Rooij Corrosion of Aluminum and Aluminum Alloys , 2011 .

[21]  R. Mishra,et al.  Friction stir processing: a novel technique for fabrication of surface composite , 2003 .

[22]  Rajiv S. Mishra,et al.  Friction Stir Welding and Processing , 2007 .

[23]  J. Murray The Al−Mg (Aluminum−Magnesium) system , 1982 .

[24]  J. C. Bailey,et al.  4.1 – Aluminium and Aluminium Alloys , 1976 .

[25]  M. M. Khruschov Principles of abrasive wear , 1974 .

[26]  H. C. H. CARPENTER,et al.  The Corrosion of Metals , 1915, Nature.