The effect of laser focus and process parameters on microstructure and mechanical properties of SLM Inconel 718

Research on the selective laser melting (SLM) method of laser powder bed fusion additive manufacturing (AM) has shown that surface and internal quality of AM parts is directly related to machine settings such as laser energy density, scanning strategies, and atmosphere. To optimize laser parameters for improved component quality, the energy density is typically controlled via laser power, scanning rate, and scanning strategy, but can also be controlled by changing the spot size via laser focal plane shift. Present work being conducted by The Aerospace Corporation was initiated after observing inconsistent build quality of parts printed using OEM-installed settings. Initial builds of Inconel 718 witness geometries using OEM laser parameters were evaluated for surface roughness, density, and porosity while varying energy density via laser focus shift. Based on these results, hardware and laser parameter adjustments were conducted in order to improve build quality and consistency. Tensile testing was also conducted to investigate the effect of build plate location and laser settings on SLM 718. This work has provided insight into the limitations of OEM parameters compared with optimized parameters towards the goal of manufacturing aerospace-grade parts, and has led to the development of a methodology for laser parameter tuning that can be applied to other alloy systems. Additionally, evidence was found that for 718, which derives its strength from post-manufacturing heat treatment, there is a possibility that tensile testing may not be perceptive to defects which would reduce component performance. Ongoing research is being conducted towards identifying appropriate testing and analysis methods for screening and quality assurance.

[1]  Barry Berman,et al.  3D printing: the new industrial revolution , 2012, IEEE Engineering Management Review.

[2]  W. Mills Fracture Toughness Variations for Alloy 718 Base Metal and Welds , 1989 .

[3]  Wei Liu,et al.  3D-imaging of selective laser melting defects in a Co–Cr–Mo alloy by synchrotron radiation micro-CT , 2015 .

[4]  Simon Ford,et al.  Additive manufacturing and sustainability: an exploratory study of the advantages and challenges , 2016 .

[5]  C. Leroux,et al.  Bone growth in rapid prototyped porous titanium implants. , 2008, Journal of biomedical materials research. Part A.

[6]  J. Corney,et al.  Grain boundary precipitation in Inconel 718 and ATI 718Plus , 2017 .

[7]  Eberhard Abele,et al.  Analysis and optimisation of vertical surface roughness in micro selective laser melting , 2015 .

[8]  Antonio Domenico Ludovico,et al.  Analysis of the molten/solidified zone in selective laser melted parts , 2014, Photonics West - Lasers and Applications in Science and Engineering.

[9]  Alaa Elwany,et al.  Effects of building orientation and heat treatment on fatigue behavior of selective laser melted 17-4 PH stainless steel , 2017 .

[10]  Christopher J. Sutcliffe,et al.  Selective laser melting of heat transfer devices , 2007 .

[11]  P. Kah,et al.  Effects of shielding gas control: welded joint properties in GMAW process optimization , 2017 .

[12]  Brent Stucker,et al.  Analysis of defect generation in Ti–6Al–4V parts made using powder bed fusion additive manufacturing processes , 2014 .

[13]  J. Dear,et al.  The effect of Ar and He shielding gas on fibre laser weld shape and microstructure in AA 2024-T3 , 2017 .

[14]  William E. Frazier,et al.  Metal Additive Manufacturing: A Review , 2014, Journal of Materials Engineering and Performance.

[15]  Moataz M. Attallah,et al.  The influence of the laser scan strategy on grain structure and cracking behaviour in SLM powder-bed fabricated nickel superalloy , 2014 .

[16]  Wei Wang,et al.  Selective laser melting of AlSi10Mg alloy: Process optimisation and mechanical properties development , 2015, Materials & Design (1980-2015).

[17]  N. Sateesh,et al.  Microstructure and Mechanical Characterization of Laser Sintered Inconel-625 Superalloy , 2014 .

[18]  Christopher J. Sutcliffe,et al.  Pressure Loss and Heat Transfer Through Heat Sinks Produced by Selective Laser Melting , 2009 .

[19]  L. Ladani,et al.  Optimizing Quality of Additively Manufactured Inconel 718 Using Powder Bed Laser Melting Process , 2016 .

[20]  HIGH DENSITY TI 6 AL 4 V VIA SLM PROCESSING : MICROSTRUCTURE AND MECHANICAL PROPERTIES , 2011 .

[21]  B. Stucker,et al.  Influence of processing parameters on the evolution of melt pool, porosity, and microstructures in Ti-6Al-4V alloy parts fabricated by selective laser melting , 2017, Progress in Additive Manufacturing.

[22]  Ryan R. Dehoff,et al.  Numerical modeling of heat-transfer and the influence of process parameters on tailoring the grain morphology of IN718 in electron beam additive manufacturing ☆ , 2016 .

[23]  Pavel Krakhmalev,et al.  Hierarchical design principles of selective laser melting for high quality metallic objects , 2015 .

[24]  Christopher J. Sutcliffe,et al.  Gas flow effects on selective laser melting (SLM) manufacturing performance , 2012 .

[25]  H. D. Carlton,et al.  The Effect of Ar and N 2 Shielding Gas on Laser Weld Porosity in Steel , Stainless Steels , and Nickel , 2015 .

[26]  Georg Schlick,et al.  Influence of the shielding gas flow on the removal of process by-products in the selective laser melting process , 2016 .

[27]  Chor Yen Yap,et al.  Review of selective laser melting : materials and applications , 2015 .

[28]  K. Mumtaz,et al.  Selective laser melting of Inconel 625 using pulse shaping , 2010 .

[29]  Thomas Imwinkelried,et al.  Mechanical properties of open-pore titanium foam. , 2007, Journal of biomedical materials research. Part A.

[30]  R. Dehoff,et al.  Effects of the microstructure and porosity on properties of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM) , 2016 .

[31]  Guha Manogharan,et al.  Making sense of 3-D printing: Creating a map of additive manufacturing products and services , 2014 .

[33]  Changmeng Liu,et al.  Parameter optimization for Ti-47Al-2Cr-2Nb in selective laser melting based on geometric characteristics of single scan tracks , 2017 .

[34]  Eugen Cicala,et al.  Experimental design approach to optimize selective laser melting of martensitic 17‐4 PH powder: part I – single laser tracks and first layer , 2012 .

[35]  R. Mines,et al.  On the Characterisation of Foam and Micro‐lattice Materials used in Sandwich Construction 1 , 2008 .

[36]  D. Gu,et al.  Effect of metal vaporization behavior on keyhole-mode surface morphology of selective laser melted composites using different protective atmospheres , 2015 .

[37]  J. Eckert,et al.  Additive Manufacturing Processes: Selective Laser Melting, Electron Beam Melting and Binder Jetting—Selection Guidelines , 2017, Materials.

[38]  L. D. Blackburn,et al.  Fracture Toughness Variations in Alloy 718 , 1988 .

[39]  I. Ashcroft,et al.  Reducing porosity in AlSi10Mg parts processed by selective laser melting , 2014 .