A novel approach for the prediction of deformation and fracture in hard coatings : Comparison of numerical modeling and nanoindentation tests

Abstract The mechanical behavior of coating systems is studied by means of a novel numerical modeling approach. The damage and fracture evolution within the coating system are modeled employing cohesive zone (CZ) regions in addition to an elasto-plastic model. The focus of this paper is on hard coatings such as (Cr,Al)N deposited by the combination of the direct current magnetron sputtering (dcMS) and the high power pulsed magnetron sputtering (HPPMS) method. The elasto-plastic properties of the coating are identified indirectly by a nanoindentation test. The morphology of the coating layer is visualized by a scanning electron microscope (SEM). Further the deformation profile after nanoindentation is measured using confocal laser scanning microscopy (CLSM). The numerical results on the measured surface profile and the required force in the nanoindentation test are compared. The coating fracture behavior is investigated by studying the influence of different parameters such as elasto-plastic properties of the coating system and the cohesive zone parameters.

[1]  S. Hao,et al.  A multi-scale model of intergranular fracture and computer simulation of fracture toughness of a carburized steel , 2010 .

[2]  M. Elices,et al.  The cohesive zone model: advantages, limitations and challenges , 2002 .

[3]  Peter Wriggers,et al.  A nonlocal cohesive zone model for finite thickness interfaces – Part II: FE implementation and application to polycrystalline materials , 2011 .

[4]  S. Reese,et al.  Prediction of fracture and damage in micro/nano coating systems using cohesive zone elements , 2017 .

[5]  T. Böhlke,et al.  Gradient crystal plasticity including dislocation-based work-hardening and dislocation transport , 2015 .

[6]  K. Bobzin,et al.  Investigation on plastic behavior of HPPMS CrN, AlN and CrN/AlN-multilayer coatings using finite element simulation and nanoindentation , 2015 .

[7]  A. Fischer-Cripps,et al.  Introduction to Contact Mechanics , 2000 .

[8]  N. Chandra,et al.  Some issues in the application of cohesive zone models for metal–ceramic interfaces , 2002 .

[9]  V. Sarin,et al.  Nanoindentation and nanoscratch properties of mullite-based environmental barrier coatings: Influence of chemical composition — Al/Si ratio , 2014 .

[10]  M. Kuna,et al.  General remarks on cyclic cohesive zone models , 2015, International Journal of Fracture.

[11]  M. Ortiz,et al.  FINITE-DEFORMATION IRREVERSIBLE COHESIVE ELEMENTS FOR THREE-DIMENSIONAL CRACK-PROPAGATION ANALYSIS , 1999 .

[12]  L. Martinu,et al.  Deposition rate enhancement in HiPIMS without compromising the ionized fraction of the deposition flux , 2013 .

[13]  R. Borst Numerical aspects of cohesive-zone models , 2003 .

[14]  Niels Bay,et al.  Application of hard coatings for blanking and piercing tools , 2011 .

[15]  A. K. Tieu,et al.  Numerical comparison between Berkovich and conical nano-indentations: Mechanical behaviour and micro-texture evolution , 2014 .

[16]  Marta Oliveira,et al.  Comparison between Berkovich, Vickers and conical indentation tests: A three-dimensional numerical simulation study , 2009 .

[17]  K. Bobzin,et al.  Influence of dcMS and HPPMS in a dcMS/HPPMS hybrid process on plasma and coating properties , 2016 .

[18]  A. Ludwig,et al.  Time- and space-resolved high-throughput characterization of stresses during sputtering and thermal processing of Al–Cr–N thin films , 2013 .

[19]  Stephan Wulfinghoff,et al.  Application of a cohesive zone element for the prediction of damage in nano/micro coating , 2015 .

[20]  G. Pharr,et al.  Cohesive interface simulations of indentation cracking as a fracture toughness measurement method for brittle materials , 2012 .

[21]  T. Clyne,et al.  A methodology for obtaining plasticity characteristics of metallic coatings via instrumented indentation , 2015 .

[22]  van der Erik Giessen,et al.  Numerical analysis of indentation-induced cracking of brittle coatings on ductile substrates , 2002 .

[23]  K. Bobzin,et al.  Investigations on Mechanical and Tribological Behavior of dcMS/HPPMS CrN and (Cr,Al)N Hard Coatings Using Nanoscratch Technique   , 2017 .

[24]  J. Mayer,et al.  On the plastic deformation of chromium-based nitride hard coatings deposited by hybrid dcMS/HPPMS: A fundamental study using nanoscratch test , 2016 .

[25]  S. Reese,et al.  Joining of the alloys AA1050 and AA5754—Experimental characterization and multiscale modeling based on a cohesive zone element technique , 2014 .

[26]  H. Espinosa,et al.  A grain level model for the study of failure initiation and evolution in polycrystalline brittle materials. Part I: Theory and numerical implementation , 2003 .

[27]  A. Ludwig,et al.  CrN/AlN nanolaminate coatings deposited via high power pulsed and middle frequency pulsed magnetron sputtering , 2014 .

[28]  V. Silberschmidt,et al.  Indentation studies in b.c.c. crystals with enhanced model of strain-gradient crystal plasticity , 2013 .

[29]  H. Zahouani,et al.  The effect of damage in the numerical simulation of a scratch test , 2007 .

[30]  O. Kraft,et al.  Fracture toughness characterization of single-crystalline tungsten using notched micro-cantilever specimens , 2016 .

[31]  G. Pharr,et al.  An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments , 1992 .

[32]  Thomas Siegmund,et al.  An analysis of the indentation test to determine the interface toughness in a weakly bonded thin film coating-substrate system , 2004 .

[33]  U. Helmersson,et al.  On the film density using high power impulse magnetron sputtering , 2010 .

[34]  Marc G. D. Geers,et al.  Multi-scale modelling of delamination through fibrillation , 2014 .

[35]  S. Fouvry,et al.  Plasma-sprayed coatings: Identification of plastic properties using macro-indentation and an inverse Levenberg–Marquardt method , 2016 .

[36]  P. Kelly,et al.  The effects of composition and pulsed biasing on chromium nitride films , 2009 .

[37]  E. Busso,et al.  On the effect of substrate properties on the indentation behaviour of coated systems , 2004 .

[38]  Yang-Tse Cheng,et al.  Delamination mechanism maps for a strong elastic coating on an elastic–plastic substrate subjected to contact loading , 2007 .

[39]  T. Kitamura,et al.  Cohesive zone criterion for cracking along the Cu/Si interface in nanoscale components , 2011 .

[40]  Nazlim Bagcivan,et al.  (Cr1 − xAlx)N: A comparison of direct current, middle frequency pulsed and high power pulsed magnetron sputtering for injection molding components , 2013 .

[41]  M. Burghammer,et al.  X-ray nanodiffraction reveals stress distribution across an indented multilayered CrN–Cr thin film , 2015 .

[42]  D. Maio,et al.  Erratum to: Measuring fracture toughness of coatings using focused-ion-beam-machined microbeams , 2005 .

[43]  Nan Li,et al.  Molecular dynamics-based cohesive zone representation of microstructure and stress evolutions of nickel intergranular fracture process: Effects of temperature , 2016 .

[44]  M. H. Aliabadi,et al.  A boundary cohesive grain element formulation for modelling intergranular microfracture in polycrystalline brittle materials , 2007 .