Deformation Mode and Microstructure on Stress Corrosion Cracking Path and Kinetics in High Temperature Water Environments
暂无分享,去创建一个
Y. Takeda | T. Shoji | Zhanpeng Lu | F. Meng | S. Yamazaki | Tichun Dan | K. Negishi
[1] Y. Takeda,et al. Characterization of microstructure and local deformation in 316NG weld heat-affected zone and stress corrosion cracking in high temperature water , 2011 .
[2] Y. Qiu,et al. The effect of roll-processing orientation on stress corrosion cracking of warm-rolled 304L stainless steel in oxygenated and deoxygenated high temperature pure water , 2010 .
[3] G. Smith,et al. Multi-scale characterization of stress corrosion cracking of cold-worked stainless steels and the influence of Cr content , 2009 .
[4] Peter L. Andresen,et al. IGSCC of non-sensitized stainless steels in high temperature water , 2008 .
[5] Z. Jiao,et al. Localized deformation and IASCC initiation in austenitic stainless steels , 2008 .
[6] Y. Takeda,et al. The dependency of the crack growth rate on the loading pattern and temperature in stress corrosion cracking of strain-hardened 316L stainless steels in a simulated BWR environment , 2008 .
[7] Y. Takeda,et al. Transient and steady state crack growth kinetics for stress corrosion cracking of a cold worked 316L stainless steel in oxygenated pure water at different temperatures , 2008 .
[8] Y. Takeda,et al. Effects of Loading Mode and Temperature on Stress Corrosion Crack Growth Rates of a Cold-Worked Type 316L Stainless Steel in Oxygenated Pure Water , 2007 .
[9] I. Thompson,et al. On the relationship between grain boundary connectivity, coincident site lattice boundaries, and intergranular stress corrosion cracking , 2004 .
[10] N. Lewis,et al. The Stress Corrosion Crack Growth Rate of Alloy 600 Heat Affected Zones Exposed to High Purity Water , 2003 .
[11] S. M. Bruemmer,et al. Study of grain boundary character along intergranular stress corrosion crack paths in austenitic alloys , 2001 .
[12] G. Was,et al. Combined effect of special grain boundaries and grain boundary carbides on IGSCC of Ni–16Cr–9Fe–xC alloys , 2001 .
[13] G. S. Was,et al. Role of Carbides in Stress Corrosion Cracking Resistance of Alloy 600 and Controlled-Purity Ni-16% Cr-9% Fe in Primary Water at 360°C , 1998 .
[14] H. Sakamoto,et al. Intergranular Stress Corrosion Crack Growth of Sensitized Type 304 Stainless Steel in a Simulated Boiling-Water Reactor Environment , 1997 .
[15] G. Was,et al. The Role of grain boundary misorientation in intergranular cracking of Ni-16Cr-9Fe in 360 °C argon and high-Purity water , 1992 .
[16] Peter L. Andresen,et al. Life prediction by mechanistic modeling and system monitoring of environmental cracking of iron and nickel alloys in aqueous systems , 1988 .
[17] Y. Qiu,et al. Effects of water chemistry and loading conditions on stress corrosion cracking of cold-rolled 316NG stainless steel in high temperature water , 2011 .
[18] M. Kikuchi,et al. SCC Growth Rates and Reference Curves for Low Carbon Stainless Steels in BWR Environment , 2004 .
[19] P. Andresen,et al. Effect of Martensite and Hydrogen on SCC of Stainless Steels and Alloy 600 , 2001 .