A novel method to prepare zinc hydroxystannate-coated inorganic fillers and its effect on the fire properties of PVC cable materials

Fire-retardant (FR) properties, including limiting oxygen index, peak rate of heat release, and smoke parameter have been measured and compared for unfilled and filled polyvinyl-chloride (PVC)-based cable formulations, containing 15 wt% amounts of uncoated and zinc-hydroxystannate (ZHS)-coated magnesium hydroxide (MH) and calcium carbonate (CaCO3) fillers at the same addition level. Of the uncoated fillers, MH was more effective at lowering flammability than CaCO3. When the ZHS coating was applied to MH and CaCO3, CaCO3 became the most effective additive at lowering PVC flammability and smoke output. POLYM. ENG. SCI., 47:1163–1169, 2007. © 2007 Society of Plastics Engineers

[1]  G. Marosi,et al.  Zinc hydroxystannate-coated metal hydroxide fire retardants: Fire performance and substrate-coating interactions , 2003 .

[2]  P. Haines,et al.  Inorganic tin compounds as flame retardants and smoke suppressants for polyester thermosets , 2000 .

[3]  Juan Carlos Cortés López,et al.  Thermal degradation of plastisols. Effect of some additives on the evolution of gaseous products , 1997 .

[4]  M. Sain,et al.  Flame retardant and mechanical properties of natural fibre–PP composites containing magnesium hydroxide , 2004 .

[5]  P. Cusack,et al.  Zinc stannate–coated fillers: Novel flame retardants and smoke suppressants for polymeric materials , 1999 .

[6]  P. Cusack,et al.  Zinc hydroxystannate as an alternative synergist to antimony trioxide in polyester resins containing halogenated flame retardants , 1997 .

[7]  F. J. Martin,et al.  Flammability of epoxy resins , 1968 .

[8]  P. Hornsby,et al.  A study of the mechanism of flame retardance and smoke suppression in polymers filled with magnesium hydroxide , 1990 .

[9]  G. Madras,et al.  Effect of Metal Oxides on Thermal Degradation of Poly(vinyl acetate) and Poly(vinyl chloride) and Their Blends , 2003 .

[10]  E. Kicko-Walczak Studies on the Mechanism of Thermal Decomposition of Unsaturated Polyester Resins with Reduced Flammability , 2004 .

[11]  E. Jakab,et al.  Effect of metals, metal oxides, and carboxylates on the thermal decomposition processes of poly (vinyl chloride) , 1999 .

[12]  A. Petsom,et al.  An oxygen index evaluation of flammability for zinc hydroxystannate and zinc stannate as synergistic flame retardants for acrylonitrile–butadiene–styrene copolymer , 2003 .

[13]  P. Hornsby,et al.  Flame retardant effects of magnesium hydroxide , 1996 .

[14]  P. Cusack,et al.  The effect of zinc hydroxystannate and zinc stannate on the fire properties of polyester resins containing additive-type halogenated flame retardants , 1993 .

[15]  Meng Feng,et al.  Thermal properties of poly(vinyl chloride)/montmorillonite nanocomposites , 2004 .