Thermophysical properties of TiB2SiC ceramics from 300 °C to 1700 °C
暂无分享,去创建一个
Zhanjun Wu | G. Shi | Zhi Wang | Zhou Wenya | Bing Xie
[1] S. Matsutomo,et al. High-frequency induction heating of Ti-coated mild steel rod for minimally invasive ablation therapy of human cancer , 2013 .
[2] Chuanzhen Huang,et al. Mechanical properties and microstructure of TiB2–TiC composite ceramic cutting tool material , 2012 .
[3] A. K. Suri,et al. Densification, characterization and oxidation studies of TiB2 – WSi2 composite , 2012 .
[4] A. K. Suri,et al. Effect of CrSi2 and HfB2 addition on densification and properties of ZrB2 , 2012 .
[5] G. Tu,et al. Characterization of the structure of TiB2/TiC composites prepared via mechanical alloying and subsequent pressureless sintering , 2012 .
[6] A. K. Suri,et al. A new TiB2 + CrSi2 composite – Densification, characterization and oxidation studies , 2010 .
[7] V. Jayaram,et al. Synthesis and Densification of Monolithic Zirconium Carbide by Reactive Hot Pressing , 2010 .
[8] V. Jayaram,et al. Low‐Temperature Densification of TiN–TiB2 Composites Through Reactive Hot Pressing with Excess Ti Additions , 2009 .
[9] Y. Sakka,et al. Influence of microstructure on the thermophysical properties of sintered SiC ceramics , 2008 .
[10] J. Narciso,et al. Fabrication and properties of graphite flakes/metal composites for thermal management applications , 2008 .
[11] V. Jayaram,et al. Reactive hot pressing of titanium nitride-titanium diboride composites at moderate pressures and temperatures , 2005 .
[12] Yu Zhou,et al. Experimental description of thermomechanical properties of carbon fiber-reinforced TiC matrix composites , 2003 .
[13] L. Matzui,et al. Influence of graphite type on electrical and thermal properties of composite materials graphite-organic compound , 2003 .
[14] C. García-Rosales,et al. Improvement of the thermo-mechanical properties of fine grain graphite by doping with different carbides , 2002 .
[15] S. Hull,et al. Structural characterisation of the -type, high pressure phase of ruthenium dioxide , 1998 .
[16] B. Basu,et al. Hot-pressed TiB2-10 wt.% TiSi2 ceramic with extremely good thermal transport properties at elevated temperatures (up to 1273 K) , 2013 .
[17] A. K. Suri,et al. Densification and oxidation behavior of a novel TiB2–MoSi2–CrB2 composite , 2013 .
[18] Bin Zou,et al. Effects of sintering additives on microstructure and mechanical properties of TiB2–WC ceramic–metal composite tool materials , 2012 .
[19] V. Jayaram,et al. Fabrication and mechanisms of densification of ZrB2-based ultra high temperature ceramics by reactive hot pressing , 2010 .
[20] K. Woo,et al. Consolidation of binderless WC–TiC by high frequency induction heating sintering , 2008 .
[21] G. Hilmas,et al. Evolution of structure during the oxidation of zirconium diboride–silicon carbide in air up to 1500 °C , 2007 .