Microstructural evolution of 6063 aluminum during friction-stir welding

The microstructural distribution associated with a hardness profile in a friction-stir-welded, age-hardenable 6063 aluminum alloy has been characterized by transmission electron microscopy (TEM) and orientation imaging microscopy (OIM). The friction-stir process produces a softened region in the 6063 Al weld. Frictional heating and plastic flow during friction-stir welding create fine recrystallized grains in the weld zone and recovered grains in the thermomechanically affected zone. The hardness profile depends greatly on the precipitate distribution and only slightly on the grain size. The softened region is characterized by dissolution and growth of the precipitates during the welding. Simulated weld thermal cycles with different peak temperatures have shown that the precipitates are dissolved at temperatures higher than 675 K and that the density of the strengthening precipitate was reduced by thermal cycles lower than 675 K. A comparison between the thermal cycles and isothermal aging has suggested precipitation sequences in the softened region during friction-stir welding.

[1]  W. Thomas,et al.  Friction stir welding for the transportation industries , 1997 .

[2]  G. A. Edwards,et al.  APFIM investigation of fine-scale precipitation in aluminium alloy 6061 , 1994 .

[3]  K. Matsuda,et al.  A metastable phase having the orthorhombic crystal lattice in an Al-1.0mass% Mg2Si-0.4mass% Si alloy , 1996 .

[4]  W. M. Thomas,et al.  Friction stir process welds aluminium alloys : The process produces low-distortion, high-quality, low-cost welds on aluminium , 1996 .

[5]  Welding of rapidly solidified Alloy 8009 (Al–8·5Fe–1·7Si–1·3V): preliminary study , 1996 .

[6]  K. Matsuda,et al.  High-resolution electron microscopy on the structure of Guinier-Preston zones in an Al-1.6 mass Pct Mg2Si alloy , 1998 .

[7]  Lawrence E Murr,et al.  A TEM study of precipitation and related microstructures in friction-stir-welded 6061 aluminium , 1998 .

[8]  D. Field,et al.  Electron backscatter diffraction and orientation imaging microscopy , 1997 .

[9]  K. Matsuda,et al.  Crystal system of rod-shaped precipitates in an Al-1.0mass%Mg2Si-0.4mass%Si alloy , 1995 .

[10]  M. Jacobs,et al.  Microanalysis of age-hardening precipitates in aluminium alloys , 1982 .

[11]  健二 松田,et al.  Al-1.0 mass%Mg2Si合金における棒状析出物の結晶構造 , 1993 .

[12]  K. Matsuda,et al.  HRTEM observation of metastable phase in Al-Mg2Si alloys. , 1997 .

[13]  D. Zhang,et al.  The quench sensitivity of cast Al-7 wt pct Si-0.4 wt pct Mg alloy , 1996 .

[14]  P. Fiorini,et al.  Effect of Si excess on the ageing behaviour of AlMg2Si 0.8% alloy , 1970 .

[15]  S. M. Allen,et al.  A calorimetric study of precipitation in commercial aluminium alloy 6061 , 1991 .

[16]  M. Jacobs The structure of the metastable precipitates formed during ageing of an Al-Mg-Si alloy , 1972 .

[17]  B. Pekkari,et al.  Friction stir welding process goes commercial , 1997 .

[18]  Hugh Shercliff,et al.  Overview No. 124 Modelling of precipitation reactions in industrial processing , 1997 .

[19]  M. W. Mahoney,et al.  Properties of friction-stir-welded 7075 T651 aluminum , 1998 .

[20]  R. Sandström,et al.  Mechanical properties of welded joints in thin walled aluminium extrusions , 1997 .

[21]  T. Sheppard Press quenching of aluminium alloys , 1988 .

[22]  K. Kunze,et al.  Orientation imaging: The emergence of a new microscopy , 1993 .

[23]  Murray W. Mahoney,et al.  Effects of friction stir welding on microstructure of 7075 aluminum , 1997 .

[24]  Lawrence E Murr,et al.  Microstructural issues in a friction-stir-welded aluminum alloy , 1998 .

[25]  Lawrence E Murr,et al.  Microstructural aspects of the friction-stir welding of 6061-T6 aluminum , 1997 .

[26]  紘一 大堀 Al-Mg-Si系合金 , 1988 .

[27]  L. Murr,et al.  Dynamic recrystallization in friction-stir welding of aluminium alloy 1100 , 1997 .

[28]  健二 松田,et al.  二段時効したAl-1.6%Mg2Si/合金の析出組織の高分解能透過型電顕観察 , 1998 .

[29]  N. Maruyama,et al.  Effect of silicon addition on the composition and structure of fine-scale precipitates in Al-Mg-Si alloys , 1997 .