Correlation of microstructure with the wear resistance and fracture toughness of white cast iron alloys

[1]  E. Romhanji,et al.  Strain hardening of austenite in Fe–Cr–C–V alloys under repeated impact , 2011 .

[2]  J. Coronado Effect of (Fe,Cr)7C3 carbide orientation on abrasion wear resistance and fracture toughness , 2011 .

[3]  Kun Liu,et al.  Sliding friction properties of austenite- and martensite-based white cast iron containing 8.5% chromium , 2010 .

[4]  M. Kazemipour,et al.  The Influence of the Matrix Microstructure on Abrasive Wear Resistance of Heat-Treated Fe–32Cr–4.5C wt% Hardfacing Alloy , 2010 .

[5]  S. Kamat,et al.  Dynamic fracture toughness of a near alpha titanium alloy Timetal 834 , 2010 .

[6]  J. Coronado,et al.  Abrasive wear study of white cast iron with different solidification rates , 2009 .

[7]  Ž. Kamberović,et al.  Matrix Microstructure and Its Micro-Analysis of Constituent Phases in As-Cast Fe-Cr-C-V Alloys , 2009 .

[8]  J. Zuno-Silva,et al.  Effect of boron on the sliding wear of directionally solidified high-chromium white irons , 2009 .

[9]  Jun Wang,et al.  Effects of high temperature and cryogenic treatment on the microstructure and abrasion resistance of a high chromium cast iron , 2009 .

[10]  J. F. Álvarez-Antolín,et al.  Identification and quantification of active manufacturing factors for graphite formation in centrifugally cast Nihard cast irons , 2008 .

[11]  H. Fu,et al.  Effect of titanium on the as-cast microstructure of hypereutectic high chromium cast iron , 2008 .

[12]  J. Gates,et al.  The role of secondary carbide precipitation on the fracture toughness of a reduced carbon white iron , 2008 .

[13]  H. Fu,et al.  Effect of heat treatment on microstructure and mechanical properties of a Ti-bearing hypereutectic high chromium white cast iron , 2008 .

[14]  Jun Wang,et al.  Effects of cryogenic treatment on microstructure and abrasion resistance of CrMnB high-chromium cast iron subjected to sub-critical treatment , 2008 .

[15]  H. Fu,et al.  Effect of titanium on the morphology of primary M7C3 carbides in hypereutectic high chromium white iron , 2007 .

[16]  P. Davami,et al.  Effects of tungsten on erosion–corrosion behavior of high chromium white cast iron , 2007 .

[17]  Haohuai Liu,et al.  Effects of deep cryogenic treatment on property of 3Cr13Mo1V1.5 high chromium cast iron , 2007 .

[18]  Wang Jun,et al.  Effect of cryogenic treatment on the matrix structure and abrasion resistance of white cast iron subjected to destabilization treatment , 2006 .

[19]  Sunghak Lee,et al.  Effects of heat treatment on wear resistance and fracture toughness of duo-cast materials composed of high-chromium white cast iron and low-chromium steel , 2006 .

[20]  D. Edmonds,et al.  Microstructural and crystallographical study of carbides in 30wt.%Cr cast irons , 2005 .

[21]  Jun Wang,et al.  Influence of secondary carbides precipitation and transformation on hardening behavior of a 15 Cr–1 Mo–1.5 V white iron , 2005 .

[22]  M. Enoki,et al.  Effect of pre-strain on fracture toughness of ductile structural steels under static and dynamic loading , 2005 .

[23]  A. Bedolla-Jacuinde,et al.  Effect of titanium on the as-cast microstructure of a 16%chromium white iron , 2005 .

[24]  Bao-luo Shen,et al.  TEM study on precipitation and transformation of secondary carbides in 16Cr–1Mo–1Cu white iron subjected to subcritical treatment , 2004 .

[25]  J. Gates,et al.  The effect of the reduction of carbon content on the toughness of high chromium white irons in the as-cast state , 2004 .

[26]  A. Bedolla-Jacuinde,et al.  Kinetics of secondary carbides precipitation in a high-chromium white iron , 2003 .

[27]  A. Bedolla-Jacuinde Microstructure of vanadium-, niobium- and titanium-alloyed high-chromium white cast irons , 2001 .

[28]  H. Çelik,et al.  Two- and three-body abrasive wear behaviour of different heat-treated boron alloyed high chromium cast iron grinding balls , 2000 .

[29]  I. Sare,et al.  Fracture toughness of high-chromium white irons: Influence of cast structure , 2000 .

[30]  J. A. Pero-Sanz,et al.  Metallographic Characterization of Hypoeutectic Martensitic White Cast Irons: Fe-C-Cr System , 1999 .

[31]  I. Sare,et al.  Effect of high temperature and sub-ambient treatments on the matrix structure and abrasion resistance of a high-chromium white iron , 1998 .

[32]  Wang Chaochang,et al.  Impact-abrasion behavior of low alloy white cast irons , 1997 .

[33]  J. Hawk,et al.  Solidification structure and abrasion resistance of high chromium white irons , 1997 .

[34]  I. Sare,et al.  The effect of heat treatment on the abrasion resistance of alloy white irons , 1997 .

[35]  G. Powell,et al.  The effect of Si on the relationship between orientation and carbide morphology in high chromium white irons , 1997 .

[36]  J. Gates,et al.  A transformation toughening white cast iron , 1997 .

[37]  O. Dogan Columnar to equiaxed transition in high Cr white iron castings , 1996 .

[38]  M. R. Ghomashchi,et al.  Microstructure-property relationships in high chromium white iron alloys , 1996 .

[39]  J. Hawk,et al.  Effect of carbide orientation on abrasion of high Cr white cast iron , 1995 .

[40]  J. Hawk,et al.  Abrasion resistance of the columnar zone in high Cr white cast irons , 1995 .

[41]  M. Fiset,et al.  The influence of vanadium on fracture toughness and abrasion resistance in high chromium white cast irons , 1994 .

[42]  G. Dunlop,et al.  Repeated impact-abrasion testing of alloy white cast irons , 1993 .

[43]  A. Wang,et al.  Impact deformation and damage of a high chromium white cast iron by spherical projectile at normal incidence , 1991 .

[44]  J. Masounave,et al.  Matrix microstructure effect on the abrasion wear resistance of high-chromium white cast iron , 1989 .

[45]  J. Pearce The use of transmission electron microscopy to study the effects of abrasive wear on the matrix structure of a high chromium cast iron , 1983 .

[46]  K. Gahr,et al.  Optimizing fracture toughness and abrasion resistance in white cast irons , 1980 .

[47]  Chongmin Kim X-ray method of measuring retained austenite in heat treated white cast irons , 1979 .

[48]  I. Sare Abrasion resistance and fracture toughness of white cast irons , 1979 .