Optimization of phase composition of Al–Cu–Mn–Zr–Sc alloys for rolled products without requirement for solution treatment and quenching

[1]  A. Pinto,et al.  The effect of Sc additions on the microstructure and age hardening behaviour of as cast Al–Sc alloys , 2012 .

[2]  W. J. Li,et al.  Heat-resistant Al–0.2Sc–0.04Zr electrical conductor , 2012 .

[3]  C. Wolverton,et al.  Role of silicon in accelerating the nucleation of Al3(Sc,Zr) precipitates in dilute Al–Sc–Zr alloys , 2012 .

[4]  S. Danis,et al.  Effect of cold rolling on precipitation processes in Al–Mn–Sc–Zr alloy , 2012 .

[5]  D. Seidman,et al.  Effect of Er additions on ambient and high-temperature strength of precipitation-strengthened Al-Zr-Sc-Si alloys , 2012 .

[6]  Kanghua Chen,et al.  A study of nanoscale Al3(Zr,Yb) dispersoids structure and thermal stability in Al–Zr–Yb alloy , 2012 .

[7]  Biao Chen,et al.  Effect of solution treatment on precipitation behaviors and age hardening response of Al–Cu alloys with Sc addition , 2011 .

[8]  D. Seidman,et al.  Effects of Yb and Zr microalloying additions on the microstructure and mechanical properties of dilute Al–Sc alloys , 2011 .

[9]  David C. Dunand,et al.  Coarsening resistance at 400 °C of precipitation-strengthened Al–Zr–Sc–Er alloys , 2011 .

[10]  D. Seidman,et al.  Precipitation evolution in Al–0.1Sc, Al–0.1Zr and Al–0.1Sc–0.1Zr (at.%) alloys during isochronal aging , 2010 .

[11]  M. Tiryakioğlu,et al.  Quench sensitivity of 2219-T87 aluminum alloy plate , 2010 .

[12]  K. Marthinsen,et al.  Precipitation kinetic of Al3(Sc,Zr) dispersoids in aluminium , 2009 .

[13]  D. Eskin Physical Metallurgy of Direct Chill Casting of Aluminum Alloys , 2008 .

[14]  H. Miura,et al.  Grain refinement in aluminum alloy 2219 during ECAP at 250 °C , 2008 .

[15]  A. Deschamps,et al.  In situ small-angle scattering study of the precipitation kinetics in an Al–Zr–Sc alloy , 2007 .

[16]  D. Eskin,et al.  Optimization of hardening of Al–Zr–Sc cast alloys , 2006 .

[17]  D. Seidman,et al.  Temporal evolution of the nanostructure of Al(Sc,Zr) alloys: Part II-coarsening of Al3(Sc1−xZrx) precipitates , 2005 .

[18]  D. Eskin,et al.  Multicomponent Phase Diagrams: Applications for Commercial Aluminum Alloys , 2005 .

[19]  E. Clouet,et al.  Precipitation kinetics of Al3Zr and Al3Sc in aluminum alloys modeled with cluster dynamics , 2005, cond-mat/0503485.

[20]  K. Marthinsen,et al.  Three dimensional atom probe investigation on the formation of Al3(Sc, Zr)-dispersoids in aluminium alloys , 2004 .

[21]  Emmanuelle A. Marquis,et al.  Nanoscale structural evolution of Al3Sc precipitates in Al(Sc) alloys , 2001 .

[22]  N. Belov Aluminium Casting Alloys with High Content of Zirconium , 1996 .

[23]  L. F. Mondolfo Aluminum alloys: Structure and properties , 1976 .