Calibration of a reflectance FTIR method for determination of dissolved CO2 concentration in rhyolitic glasses

Abstract A technique based upon infrared reflectance spectroscopy is developed as an alternative to the Fourier transform infrared (FTIR) transmission method for the quantitative measurement of dissolved molecular carbon dioxide in aluminosilicate glasses. The technique has the advantage that only a single sample surface need be polished, and no thickness measurement is necessary. The reflectance spectrum is analyzed by Kramers–Kronig relations or classical oscillator analysis to yield the optical constants and the absorption coefficient at 2350 cm −1 , due to the asymmetric stretching (ν 3 ) vibration of molecular CO 2 . The value obtained is in excellent agreement with values obtained by the transmission FTIR technique for a suite of rhyolitic glasses. For practical application of the method to rhyolites, an empirical correlation is developed between the normalized change in reflectance at 2350 cm −1 and the CO 2 content, up to ∼0.40 wt%.

[1]  M. S. Paterson,et al.  The determination of hydroxyl by infrared absorption in quartz, silicate glasses and similar materials , 1982 .

[2]  William H. Press,et al.  Numerical Recipes: FORTRAN , 1988 .

[3]  J. Blank,et al.  Experimental studies of carbon dioxide in silicate melts; solubility, speciation, and stable carbon isotope behavior , 1994 .

[4]  Armand Hadni,et al.  Essentials of modern physics applied to the study of the infrared , 1967 .

[5]  R. Fogel,et al.  The solubility of carbon dioxide in rhyolitic melts; a quantitative FTIR study , 1990 .

[6]  R. Lange The effect of H 2 O, CO 2 and F on the density and viscosity of silicate melts , 1994 .

[7]  E. Stolper,et al.  The speciation of carbon dioxide in sodium aluminosilicate glasses , 1985 .

[8]  E. Stolper,et al.  An Experimental Study of Water and Carbon Dioxide Solubilities in Mid-Ocean Ridge Basaltic Liquids. Part I: Calibration and Solubility Models , 1995 .

[9]  A. T. Anderson,et al.  Quantification of pre-eruptive exsolved gas contents in silicic magmas , 1995, Nature.

[10]  S. Newman,et al.  Measurement of water in rhyolitic glasses; calibration of an infrared spectroscopic technique , 1986 .

[11]  P. McMillan,et al.  Solubility, speciation and dissolution mechanisms for CO2 in melts on the NaAlO2–SiO2 join , 1999 .

[12]  Shiv k. Sharma,et al.  The effect of bulk composition on the speciation of water in submarine volcanic glasses , 1992 .

[13]  Roger H. French,et al.  Quantitative, FFT-Based, Kramers-Krönig Analysis for Reflectance Data , 1989 .

[14]  Paul F. McMillan,et al.  FTIR micro-reflectance measurements of the CO32– ion content in basanite and leucitite glasses , 1996 .

[15]  Marie C. Johnson,et al.  Pre-eruptive volatile contents of magmas , 1994 .

[16]  I. Carmichael The iron-titanium oxides of salic volcanic rocks and their associated ferromagnesian silicates , 1966 .

[17]  E. Stolper,et al.  Dissolved carbon dioxide in basaltic glasses: concentrations and speciation , 1986 .

[18]  P. McMillan,et al.  Analytical methods for volatiles in glasses , 1994 .

[19]  S. Newman,et al.  Solubility of carbon dioxide in albitic melt , 1987 .

[20]  Andrei M. Efimov,et al.  Optical Constants of Inorganic Glasses , 1995 .