Effects of ion beam etching of fused silica substrates on the laser-induced damage properties of antireflection coatings at 355 nm

Abstract Antireflection (AR) coatings are deposited on UV grade fused silica substrates, which are cleaned in the dual ion beam sputtering device. Compared to ultrasonic and acid etching cleaning progress, ion beam etching improves the laser-induced damage threshold (LIDT) of substrates and AR coatings significantly at 355 nm. Ion beam etching declines the low LIDT defects drastically and removes lots of the impurity elements (Ce, Fe, K, and Na). Roughness test shows that the AR coatings and substrates with ion beam etching are very flat and of low roughness. Ion beam etching reduces the density of deep defect from substrates greatly. Damage morphologies show double layers delamination, which is explained via calculation of layer stress. This study will be helpful for preparation of high LIDT optical coatings.

[1]  G. Wei,et al.  Antireflective coatings with adjustable transmittance and high laser-induced damage threshold prepared by deposition of magnesium fluoride nanoparticles , 2015 .

[2]  Jin Huang,et al.  Reaction ion etching process for improving laser damage resistance of fused silica optical surface. , 2016, Optics express.

[3]  D. Ristau Laser-induced damage in optical materials , 2014 .

[4]  C D Boley,et al.  Impact of laser-contaminant interaction on the performance of the protective capping layer of 1 ω high-reflection mirror coatings. , 2015, Applied optics.

[5]  Linas Smalakys,et al.  Sculptured anti-reflection coatings for high power lasers , 2017 .

[6]  Regina Soufli,et al.  Substrate and coating defect planarization strategies for high-laser-fluence multilayer mirrors , 2015 .

[7]  Minglun Gong,et al.  Over 8 W high peak power UV laser with a high power Q-switched Nd:YVO4 oscillator and the compact extra-cavity sum-frequency mixing , 2009 .

[8]  P. Miller,et al.  Particle damage sources for fused silica optics and their mitigation on high energy laser systems. , 2017, Optics express.

[9]  Wei Li,et al.  Preparation and stability study of broadband anti-reflection coatings and application research for CdTe solar cell , 2018 .

[10]  K. L. Mittal,et al.  Developments in Surface Contamination and Cleaning: Methods for Surface Cleaning : Volume 9 , 2016 .

[11]  Qinmin Pan,et al.  Synthesis and characterization of nanostructured poly(methyl methacrylate) for antireflection coating , 2014 .

[12]  In Situ Fabrication of Density-Controlled ZnO Nanorod Arrays on a Flexible Substrate Using Inductively Coupled Plasma Etching and Microwave Irradiation , 2008 .

[13]  K. Juškevičius,et al.  Argon plasma etching of fused silica substrates for manufacturing high laser damage resistance optical interference coatings , 2017 .

[14]  Stephen R. Forrest,et al.  Enhanced light out-coupling of organic light-emitting devices using embedded low-index grids , 2008 .

[15]  Jérôme Néauport,et al.  Effects of deep wet etching in HF/HNO3 and KOH solutions on the laser damage resistance and surface quality of fused silica optics at 351 nm. , 2017, Optics express.

[16]  Zongfu Yu,et al.  Producing air-stable monolayers of phosphorene and their defect engineering , 2016, Nature Communications.

[17]  Liqiang Cao,et al.  Deep dry etching of fused silica using C4F8/Ar inductively coupled plasmas , 2016, Journal of Materials Science: Materials in Electronics.

[18]  K. Juškevičius,et al.  Optical resistance and spectral properties of anti-reflective coatings deposited on LBO crystals by ion beam sputtering , 2011 .

[19]  A. Seitsonen,et al.  Atomically precise bottom-up fabrication of graphene nanoribbons , 2010, Nature.

[20]  L. L. Wong,et al.  HF‐Based Etching Processes for Improving Laser Damage Resistance of Fused Silica Optical Surfaces , 2011 .

[21]  G. Oehrlein,et al.  Investigation of thin oxide layer removal from Si substrates using an SiO2 atomic layer etching approach: the importance of the reactivity of the substrate , 2017 .

[22]  K. Oh,et al.  Extreme wettability of nanostructured glass fabricated by non-lithographic, anisotropic etching , 2015, Scientific Reports.

[23]  Laurent Gallais,et al.  Investigation of nanoprecursors threshold distribution in laser-damage testing , 2005 .

[24]  Deepak,et al.  Improving the contrast ratio of OLED displays: An analysis of various techniques , 2012 .

[25]  S. Papernov,et al.  Localized absorption effects during 351 nm, pulsed laser irradiation of dielectric multilayer thin films , 1997 .

[26]  H. Dai,et al.  Narrow graphene nanoribbons from carbon nanotubes , 2009, Nature.

[27]  Jun Shen,et al.  Ultraviolet laser-induced damage on fused silica substrate and its sol-gel coating. , 2012, Optics letters.