The influence of interfacial failure on the tensile S–N response of aged Arcan joints

[1]  Jingxin Na,et al.  Influence of temperature and humidity on the fatigue behaviour of adhesively bonded CFRP/aluminium alloy joints , 2021, The Journal of Adhesion.

[2]  R. Carbas,et al.  Cyclic ageing of adhesive materials , 2021, The Journal of Adhesion.

[3]  R. Carbas,et al.  Effect of Water Ingress on the Mechanical and Chemical Properties of Polybutylene Terephthalate Reinforced with Glass Fibers , 2021, Materials.

[4]  L. Silva,et al.  Experimental and numerical analysis of cyclic aging in an epoxy-based adhesive , 2020, Polymer Testing.

[5]  Wang Guangbin,et al.  Effects of hygrothermal aging on the mechanical properties of aluminum alloy adhesive joints for high-speed train applications , 2020, The Journal of Adhesion.

[6]  L. Silva,et al.  Review on the effect of moisture and contamination on the interfacial properties of adhesive joints , 2020 .

[7]  L. F. Silva,et al.  Influence of mode mixity and loading conditions on the fatigue crack growth behaviour of an epoxy adhesive , 2020, Fatigue & Fracture of Engineering Materials & Structures.

[8]  E. Marques,et al.  Fatigue performance of single lap joints with CFRP and aluminium substrates prior and after hygrothermal aging , 2019, Fatigue & Fracture of Engineering Materials & Structures.

[9]  L. F. Silva,et al.  Effect of hygrothermal aging on the quasi-static behaviour of CFRP joints varying the overlap length , 2019, Composite Structures.

[10]  M. Ayatollahi,et al.  Impact of geometry on the critical values of the stress intensity factor of adhesively bonded joints , 2017 .

[11]  L. D. da Silva,et al.  Hygrothermal aging of an adhesive reinforced with microparticles of cork , 2015 .

[12]  B. Carlson,et al.  Experimental study of initial strengths and hygrothermal degradation of adhesive joints between thin aluminum and steel substrates , 2013 .

[13]  H. Koguchi,et al.  Analysis of the stress singularity field at a vertex in 3D-bonded structures having a slanted side surface , 2010 .

[14]  I. Ashcroft,et al.  Modelling interfacial degradation using interfacial rupture elements , 2003 .

[15]  L. Silva,et al.  Effect of Humidity on The Fatigue Behaviour of Adhesively Bonded Aluminium Joints , 2017 .

[16]  Andreas Öchsner,et al.  Handbook of adhesion technology , 2011 .