Investigation of macrostructure, microstructure, and hot cracking susceptibility of laser-welded Inconel-718 superalloy under various post-cold treatment environments

[1]  M. Rezaei,et al.  The effect of pre-cold treatment on microstructure, weldability and mechanical properties in laser welding of superalloys , 2018, Journal of Manufacturing Processes.

[2]  J. Andersson,et al.  Hot cracking in cast alloy 718 , 2018 .

[3]  Z. Deng,et al.  Effect of water depth on weld quality and welding process in underwater fiber laser welding , 2017 .

[4]  F. Lu,et al.  Dendritic microstructure and hot cracking of laser additive manufactured Inconel 718 under improved base cooling , 2016 .

[5]  Chenxi Liu,et al.  Effect of base metal and welding speed on fusion zone microstructure and HAZ hot-cracking of electron-beam welded Inconel 718 , 2016 .

[6]  WU C.S.,et al.  Visual Sensing of the Physical Process During Underwater Wet , 2016 .

[7]  Xueming Hua,et al.  Controlling hot cracking in Ni-based Inconel-718 superalloy cast sheets during tungsten inert gas welding , 2015 .

[8]  K. P. Rao,et al.  Microstructural characterization of liquid nitrogen cooled Alloy 718 fusion zone , 2014 .

[9]  A. Scotti,et al.  The effect of metal transfer stability (spattering) on fume generation, morphology and composition in short-circuit MAG welding , 2014 .

[10]  N. S. Prasad,et al.  Studies on multipass welding with trailing heat sink considering phase transformation , 2014 .

[11]  S. H. Seyedein,et al.  Modern fiber laser beam welding of the newly-designed precipitation-strengthened nickel-base superalloys , 2014 .

[12]  M. Kamaraj,et al.  Effect of weld cooling rate on Laves phase formation in Inconel 718 fusion zone , 2014 .

[13]  P. Wanjara,et al.  Microstructure and hardness of fiber laser deposited Inconel 718 using filler wire , 2013 .

[14]  S. H. Seyedein,et al.  Microstructural, mechanical and weldability assessments of the dissimilar welds between γ′- and γ″-strengthened nickel-base superalloys , 2013 .

[15]  Sushant K. Manwatkar,et al.  Effect of Welding Processes (GTAW & EBW) and Solutionizing Temperature on Microfissuring Tendency in Inconel 718 Welds , 2012 .

[16]  O. Ojo,et al.  Single pass laser joining of Inconel 718 superalloy with filler , 2011 .

[17]  H. Fu,et al.  Influence of directional solidification variables on the microstructure and crystal orientation of AM3 under high thermal gradient , 2010 .

[18]  N. Ünlü,et al.  A Study on Laser Beam Welding (LBW) Technique: Effect of Heat Input on the Microstructural Evolution of Superalloy Inconel 718 , 2010 .

[19]  Xinjin Cao,et al.  Effect of pre- and post-weld heat treatment on metallurgical and tensile properties of Inconel 718 alloy butt joints welded using 4 kW Nd:YAG laser , 2009 .

[20]  Jian-xin Dong,et al.  AN INVESTIGATION OF MICROSEGREGATION AND LIQUID DENSITY REDISTRIBUTION DURING SOLIDIFICATION OF INCONEL 718 , 2009 .

[21]  F. Matsuda,et al.  Effect of shielding conditions of local dry cavity on weld quality in underwater Nd:YAG laser welding , 2006 .

[22]  G. Reddy,et al.  Microstructure and tensile properties of Inconel 718 pulsed Nd-YAG laser welds , 2005 .

[23]  G. Reddy,et al.  Residual stresses in Inconel 718 electron beam welds , 2004 .

[24]  Fukuhisa Matsuda,et al.  Relationship between weld quality and optical emissions in underwater Nd: YAG laser welding , 2004 .

[25]  J. Lippold,et al.  Liquation phenomena in the simulated heat-affected zone of alloy 718 after multiple postweld heat treatment cycles , 2003 .

[26]  Structural Steels,et al.  Welding Metallurgy of , 1987 .

[27]  A. Pineau,et al.  The effect of microstructure and environment on the crack growth behaviour of Inconel 718 alloy at 650 °C under fatigue, creep and combined loading , 1982 .

[28]  K. Masubuchi,et al.  Mechanisms of rapid cooling in underwater welding , 1979 .