The Effects of Al‐5Ti‐1B Grain Refiner and Heat Treatment on the Microstructure and Dry Sliding Wear Behavior of a New Developed Super High‐Strength Aluminum Alloy

[1]  A. Crosky,et al.  Secondary ageing in an aluminium alloy 7050 , 2008 .

[2]  R. Mishra,et al.  Structure-property correlations in Al 7050 and Al 7055 high-strength aluminum alloys , 2008 .

[3]  F. Gracia,et al.  Conduction processes in tin-and silicon-phthalocyanine thin films , 2007 .

[4]  Li Jie,et al.  Single-aging characteristics of 7055 aluminum alloy , 2007 .

[5]  Q. Meng,et al.  The microstructural evolution of an Al–Zn–Mg–Cu alloy during homogenization , 2006 .

[6]  Jie Dong,et al.  A new way to cast high-alloyed Al–Zn–Mg–Cu–Zr for super-high strength and toughness , 2006 .

[7]  Ping Li,et al.  The constituents in Al–10Zn–2.5Mg–2.5Cu aluminum alloy , 2005 .

[8]  C. Mondal,et al.  On the nature of T(Al2Mg3Zn3) and S(Al2CuMg) phases present in as-cast and annealed 7055 aluminum alloy , 2005 .

[9]  R. Samur,et al.  Tribological Behaviour of Combined Coatings Deposited on Aluminium , 2004 .

[10]  A. L. Greer,et al.  The effect of the size distribution of inoculant particles on as-cast grain size in aluminium alloys , 2004 .

[11]  Jie Dong,et al.  Effect of low-frequency electromagnetic casting on the castability, microstructure, and tensile properties of direct-chill cast Al-Zn-Mg-Cu alloy , 2004 .

[12]  L. Rokhlin,et al.  Investigation of phase equilibria in alloys of the Al-Zn-Mg-Cu-Zr-Sc system , 2004 .

[13]  A. N. Khramov,et al.  Investigation of quaternary Al-based quasicrystal thin films for corrosion protection , 2004 .

[14]  Kazuhiro Nakata,et al.  Fe–Al composite layers on aluminum alloy formed by laser surface alloying with iron powder , 2003 .

[15]  G. Lu,et al.  Effects of low-frequency electromagnetic field on microstructures and macrosegregation of continuous casting 7075 aluminum alloy , 2003 .

[16]  N. Chen,et al.  In situ formation of MoSi2/SiC composite coating on pure Al by laser cladding , 2003 .

[17]  A. Okada,et al.  Surface modification of A2014 Al alloy using a pulse-current pressure sintering process , 2003 .

[18]  M. Ushio,et al.  Effect of Fe content on wear resistance of thermal-sprayed Al–17Si–XFe alloy coating on A6063 Al alloy substrate , 2003 .

[19]  K. Mori,et al.  Lining of light metals with hard powders using shot peening , 2002 .

[20]  J. Dutkiewicz,et al.  The effect of plastic deformation on structure and properties of chosen 6000 series aluminium alloys , 2002 .

[21]  S. A. Kori,et al.  Grain refinement of aluminium and its alloys by heterogeneous nucleation and alloying , 2002 .

[22]  T. Yue,et al.  Laser surface alloying of NiCrSiB on Al6061 aluminium alloy , 2001 .

[23]  A. Edrisy,et al.  Wear of thermal spray deposited low carbon steel coatings on aluminum alloys , 2001 .

[24]  Dongyang Li,et al.  Improvement in the resistance of aluminum with yttria particles to sliding wear in air and in a corrosive medium , 2001 .

[25]  Masahiro Okumiya,et al.  Surface modification of aluminum using ion nitriding and fluidized bed , 2001 .

[26]  T. Kubo,et al.  Formation of metal matrix composite layer on aluminum alloy with TiC-Cu powder by laser surface alloying process , 2001 .

[27]  Q. Xue,et al.  Duplex treatment for surface improvement of 2024 Al , 2001 .

[28]  N. Dahotre,et al.  Microstructural and tribological characterization of an A-356 aluminum alloy superficially modified by laser alloying , 2000 .

[29]  Thierry Czerwiec,et al.  Low-temperature plasma-assisted nitriding , 2000 .

[30]  P. Dearnley,et al.  The sliding wear resistance and frictional characteristics of surface modified aluminium alloys under extreme pressure , 1999 .

[31]  Murat Çağlar Baydoğan,et al.  The effect of deformation before ageing on the wear resistance of an aluminium alloy , 1999 .

[32]  T. Srivatsan,et al.  Microstructure, tensile deformation and fracture behaviour of aluminium alloy 7055 , 1997 .

[33]  K. Rie,et al.  Plasma assisted CVD for low temperature coatings to improve the wear and corrosion resistance , 1996 .

[34]  G. Jones,et al.  Factors affecting the grain-refinement of aluminum using titanium and boron additives , 1976 .