Synthesis and characterization of micro-spherical tungsten-molybdenum alloy particles using spray drying combined with microwave assisted calcination process

[1]  D. Bressler,et al.  Recent developments in microwave-assisted thermal conversion of biomass for fuels and chemicals , 2018, Renewable and Sustainable Energy Reviews.

[2]  Jinshu Wang,et al.  Effect of yttrium doping on the formation and stability of β‑tungsten powder , 2018 .

[3]  Taha Rostamzadeh,et al.  Formation of molybdate organic-hybrids and exfoliated molybdate nanosheets , 2017 .

[4]  Jialin Chen,et al.  Synthesis and characterization of high-purity micro-spherical (NH4)2RuCl6 particles using chemical separation combined with spray dried techniques , 2017 .

[5]  P. Veronesi,et al.  High entropy alloys obtained by field assisted powder metallurgy route: SPS and microwave heating , 2017 .

[6]  M. Wen,et al.  Synthesis of high-purity micro-spherical ruthenium particles by chemical refining method , 2016 .

[7]  M. Suk,et al.  Porous Mo–30wt.% W alloys synthesized from camphene/MoO3–WO3 slurry by freeze drying and sintering process , 2015 .

[8]  P. Sahoo,et al.  Consolidation behavior of W–20–40 wt.% Mo nanoalloys synthesized by thermal decomposition method , 2015 .

[9]  Lei Lu,et al.  Effect of rare earth element cerium on preparation of tungsten powders , 2015 .

[10]  E. Bobicki,et al.  Microwave heating of ultramafic nickel ores and mineralogical effects , 2014 .

[11]  G. Schreiber,et al.  Spark plasma sintering of Mo–W powders prepared by mechanical alloying , 2013 .

[12]  B. S. Murty,et al.  Dilatometric analysis on shrinkage behavior during non-isothermal sintering of nanocrystalline tungsten mechanically alloyed with molybdenum , 2012 .

[13]  A. K. Suri,et al.  Sintering kinetics study of mechanically alloyed nanocrystalline Mo-30 wt.% W , 2011 .

[14]  Kikuo Okuyama,et al.  Progress in developing spray-drying methods for the production of controlled morphology particles: From the nanometer to submicrometer size ranges , 2011 .

[15]  A. K. Suri,et al.  Studies on the synthesis of a Mo–30 wt% W alloy by non-conventional approaches , 2010 .

[16]  B. S. Murty,et al.  On sinterability of nanostructured W produced by high-energy ball milling , 2007 .

[17]  M. Nagano,et al.  Gas sensing properties of a stabilized zirconia-based sensor with a porous MoO3 electrode prepared from a molybdenum polyoxometallate–alkylamine hybrid film , 2006 .

[18]  M. Abdullah,et al.  Preparation of functional nanostructured particles by spray drying , 2006 .

[19]  X. Liu,et al.  Thermal response of plasma sprayed tungsten coating to high heat flux , 2004 .

[20]  G. Greene,et al.  Vaporization of tungsten in flowing steam at high temperatures , 2001 .