Deformation behavior and enhanced plasticity of Ti-based metallic glasses with notches

The plasticity of Ti-based metallic glasses with different aspect ratios can be improved by introducing two semicircular notches on the edges of the samples, owing to the interactions of shear bands (SBs) under conventional compression tests. The interaction of SBs can be ascribed to the easy initiation of SBs around the notches due to the large stress gradient, and the consequent blocking effect of notches on the propagation of shear bands. Additionally, the current findings provide a new way to understand the physical nature for the plastic deformation behavior of some brittle metallic glasses and supply an effective approach to enhance the plasticity to some extent.

[1]  Frans Spaepen,et al.  A microscopic mechanism for steady state inhomogeneous flow in metallic glasses , 1977 .

[2]  C. Pampillo Flow and fracture in amorphous alloys , 1975 .

[3]  S. Poon,et al.  Ductile titanium-based glassy alloy ingots , 2005 .

[4]  Remo Guidieri Res , 1995, RES: Anthropology and Aesthetics.

[5]  Douglas C. Hofmann,et al.  Designing metallic glass matrix composites with high toughness and tensile ductility , 2008, Nature.

[6]  J. Eckert,et al.  Fracture mechanism of some brittle metallic glasses , 2009 .

[7]  A. Argon Plastic deformation in metallic glasses , 1979 .

[8]  S. Hong,et al.  Enhancement of plasticity in Zr-base bulk metallic glass by soft metal plating , 2009 .

[9]  Weihua Wang,et al.  Bulk metallic glasses , 2004 .

[10]  G. Ravichandran,et al.  Pressure-dependent flow behavior of Zr_41.2Ti_13.8Cu_12.5Ni_10Be_22.5 bulk metallic glass , 2003 .

[11]  W. Johnson,et al.  Processing, microstructure and properties of ductile metal particulate reinforced Zr57Nb5Al10Cu15.4Ni12.6 bulk metallic glass composites , 2002 .

[12]  J. Shen,et al.  Formation of nanowaves in compressive fracture of a less-brittle bulk metallic glass , 2006 .

[13]  A. Argon,et al.  The mechanism of fracture in glassy materials capable of some inelastic deformation , 1976 .

[14]  L. Dai,et al.  Energy dissipation in fracture of bulk metallic glasses via inherent competition between local softening and quasi-cleavage , 2008 .

[15]  Z. Zhang,et al.  Shear deformation and plasticity of metallic glass under multiaxial loading , 2008 .

[16]  F. Wu,et al.  Size-dependent shear fracture and global tensile plasticity of metallic glasses , 2009 .

[17]  Nb,et al.  Size Effect on Shear Fracture and Fragmentation of a Fe57.6Co14.4B19.2Si4.8Nb4 Bulk Metallic Glass , 2008 .

[18]  J. Eckert,et al.  Effect of aspect ratio on the compressive deformation and fracture behaviour of Zr-based bulk metallic glass , 2005 .

[19]  H. Bei,et al.  Softening caused by profuse shear banding in a bulk metallic glass. , 2006, Physical review letters.

[20]  Zushu Hu,et al.  Mechanical properties of tungsten fiber reinforced ZrAlNiCuSi metallic glass matrix composite , 2002 .

[21]  Keith C. C. Chan,et al.  Instability of crack propagation in brittle bulk metallic glass , 2008 .

[22]  T. Hufnagel,et al.  Mechanical behavior of amorphous alloys , 2007 .

[23]  Hays,et al.  Microstructure controlled shear band pattern formation and enhanced plasticity of bulk metallic glasses containing in situ formed ductile phase dendrite dispersions , 2000, Physical review letters.

[24]  H. Chen,et al.  Thermodynamic considerations on the formation and stability of metallic glasses , 1974 .

[25]  Andrew G. Glen,et al.  APPL , 2001 .

[26]  J. Shen,et al.  Shear deformation capability of different metallic glasses , 2008 .

[27]  Yat Li,et al.  Size-dependent “malleable-to-brittle” transition in a bulk metallic glass , 2008 .

[28]  M. Demetriou,et al.  Development of tough, low-density titanium-based bulk metallic glass matrix composites with tensile ductility , 2008, Proceedings of the National Academy of Sciences.

[29]  Ludwig Schultz,et al.  Novel Ti-base nanostructure–dendrite composite with enhanced plasticity , 2003, Nature materials.

[30]  W. Wang,et al.  Making metallic glasses plastic by control of residual stress , 2006, Nature materials.

[31]  J. Lewandowski,et al.  Effects of annealing and specimen geometry on dynamic compression of a Zr-based bulk metallic glass , 2007 .

[32]  Hugh Alan Bruck,et al.  Quasi-static constitutive behavior of Zr41.25Ti13.75Ni10Cu12.5Be22.5 bulk amorphous alloys , 1994 .

[33]  Huajian Gao,et al.  An instability index of shear band for plasticity in metallic glasses , 2009 .

[34]  A. Inoue Stabilization of metallic supercooled liquid and bulk amorphous alloys , 2000 .