Measurement of positron reemission from thin single-crystal W(100) films.
暂无分享,去创建一个
Epitaxial thin single-crystal (100) tungsten films 1000, 2500, and 5000 A thick have been fabricated by high-vacuum electron-beam evaporation. These films were subsequently used as thin-film moderators for the study of the positron-transmission-reemission process with a variable-energy (0--80 keV) monoenergetic positron beam in an ultrahigh-vacuum system. The films were shown to be routinely cleanable by heating first in oxygen (10/sup -6/ Torr) and then in vacuum (10/sup -9/ Torr). Transmission and back reemission of slow positrons from these surfaces was observed. The positron work function, phi/sub +/ has been determined to be approx. =3.0 eV ( +- 0.3 eV). The transmission slow positrons were emitted in a narrow cone with a full width at half maximum of approx. =30/sup 0/ consistent with the angular distribution of back-reemission positrons. The reemitted yields as a function of incident positron energy were found to be very different between forward reemission and back reemission. The maximum forward-reemission yields were 18% for 1000-A-thick W film and 12% for 2500-A-thick W film at 5 and 10 keV optimum incident positron energies, respectively. These results show that one can use thin single-crystal tungsten films as positron moderators or remoderators.