Atomic Layer Deposition of Platinum Thin Films

Platinum thin films were grown at 300 °C by atomic layer deposition (ALD) using (methylcyclopentadienyl)trimethylplatinum (MeCpPtMe3) and oxygen as precursors. The films had excellent uniformity, low resistivity, and low-impurity contents. Structural studies by X-ray diffraction showed that the films were strongly (111) oriented. Growth rates of 0.45 A cycle-1 were obtained with 4 s total cycle times. The film thickness was found to linearly depend on the number of the reaction cycles. Also, the possible reaction mechanism is discussed.