End-of-life and replacement strategies for RTV silicone rubber coatings

The paper provides several methods to assess the condition of RTV coated porcelain/toughened glass insulators in the field. Visual observations of arcing and audible corona are the first indications that signal changes to the coating have taken place. It emphasizes that in the absence of reliable data one can use observations based on hydrophobicity to evaluate when maintenance or replacement of the coated insulators is necessary. Life extension strategies are suggested. It also demonstrates that there are differences in the hydrophobicity characteristics among commercially available coatings, and these can be quantified using standard laboratory techniques. Field experience suggests that the life of the RTV coatings can exceed 10 years even under the severest conditions of pollution.

[1]  E. Cherney,et al.  Aging Characteristics of RTV Silicone Rubber Insulator Coatings , 2008, IEEE Transactions on Dielectrics and Electrical Insulation.

[2]  Zhicheng Guan,et al.  Durability of RTV-coated insulators used in subtropical areas , 2011, IEEE Transactions on Dielectrics and Electrical Insulation.

[3]  R. Gorur,et al.  Surface hydrophobicity of polymers used for outdoor insulation , 1990 .

[4]  M. Owen,et al.  Synthesis and properties of silicones and silicone-modified materials , 2003 .

[5]  R.S. Gorur,et al.  Evaluating station post insulator performance from electric field calculations , 2008, IEEE Transactions on Dielectrics and Electrical Insulation.

[6]  S. Low,et al.  Rain and contamination tests on HVDC wall bushings with and without RTV coatings , 1991 .

[7]  M. Chaudhury,et al.  Hydrophobicity loss and recovery of silicone HV insulation , 1999, IEEE Transactions on Dielectrics and Electrical Insulation.

[8]  R. Hackam,et al.  Chemical changes at the surface of RTV silicone rubber coatings on insulators during dry-band arcing , 1994 .

[9]  E. A. Cherney,et al.  RTV silicone-a high tech solution for a dirty insulator problem , 1995 .

[10]  Yitzhak Apeloig,et al.  The chemistry of organic silicon compounds , 1989 .

[11]  T. Sorqvist Long-term field experience with RTV coated porcelain insulators , 2000, Conference Record of the 2000 IEEE International Symposium on Electrical Insulation (Cat. No.00CH37075).

[12]  S. Boggs,et al.  Field and laboratory aging of RTV silicone insulator coatings , 2000 .

[13]  R. S. Gorur,et al.  Accelerated aging and flashover tests on 138 kV nonceramic line post insulators , 1993 .

[14]  Z. Jia,et al.  Development of RTV Silicone Coatings in China: Overview and Bibliography [Feature article] , 2008, IEEE Electrical Insulation Magazine.

[15]  R. J. Hill Laboratory analysis of naturally aged silicone rubber polymer insulators from contaminated environments, 138 to 145 kV , 1994, Proceedings of IEEE/PES Transmission and Distribution Conference.

[16]  R. Gorur,et al.  RTV silicone rubber pre-coated ceramic insulators for transmission lines , 2013, IEEE Transactions on Dielectrics and Electrical Insulation.

[17]  Licheng Li,et al.  Mechanism of contaminant accumulation and flashover of insulator in heavily polluted coastal area , 2010, IEEE Transactions on Dielectrics and Electrical Insulation.

[18]  S. Boggs,et al.  Degradation of a silicone-based coating in a substation application , 1999 .