The characteristics and reduction of porosity in high-power laser welds of thick AISI 304 plate

[1]  Kebing Zhang,et al.  Fiber laser welding of thick AISI 304 plate in a horizontal (2G) butt joint configuration , 2017 .

[2]  R. Kovacevic,et al.  High power laser welding of thick steel plates in a horizontal butt joint configuration , 2016 .

[3]  X. Shao,et al.  Dynamics of vapor plume in transient keyhole during laser welding of stainless steel: Local evaporation, plume swing and gas entrapment into porosity , 2016 .

[4]  Yue Wu,et al.  Influence of absorbed nitrogen on microstructure and corrosion resistance of 2205 duplex stainless steel joint processed by fiber laser welding , 2016 .

[5]  Xianfeng Shen,et al.  Comparison of processing window and porosity distribution in laser welding of 10 mm thick 30CrMnSiA ultrahigh strength between flat (1G) and horizontal (2G) positions , 2016 .

[6]  T. Chao,et al.  The Effects of Entrainment on Pore Shape in Keyhole Mode Welding , 2015 .

[7]  F. Lu,et al.  Investigation on the effects of shielding gas on porosity in fiber laser welding of T-joint steels , 2015 .

[8]  O. Ola,et al.  Keyhole-induced porosity in laser-arc hybrid welded aluminum , 2015 .

[9]  Jesper Sundqvist,et al.  Laser Welding Of Duplex Stainless Steel With Nitrogen As Shielding Gas , 2015 .

[10]  S. Katayama,et al.  The influence of various factors on the geometric profile of laser lap welded T-joints , 2014 .

[11]  R. Kovacevic,et al.  Pore formation mechanism and its mitigation in laser welding of AZ31B magnesium alloy in lap joint configuration , 2014 .

[12]  Anthony J. Martin,et al.  Effect of Travel Speed and Beam Focus on Porosity in Alloy 690 Laser Welds , 2012 .

[13]  Susumu Tsukamoto,et al.  High speed imaging technique Part 2 – High speed imaging of power beam welding phenomena , 2011 .

[14]  S. Katayama,et al.  High quality welding of stainless steel with 10 kW high power fibre laser , 2009 .

[15]  Stefano Beretta,et al.  Estimate of maximum pore size in keyhole laser welding of carbon steel , 2009 .

[16]  K. Mills,et al.  Determination of the surface tension of liquid stainless steel , 2005 .

[17]  S. Jeng,et al.  Porosity reduction in Nd–YAG laser welding of stainless steel and inconel alloy by using a pulsed wave , 2005 .

[18]  Seiji Katayama,et al.  Development of porosity prevention procedures during laser welding , 2003, International Congress on Laser Advanced Materials Processing.

[19]  Akira Matsunawa,et al.  Prevention of welding defect by side gas flow and its monitoring method in continuous wave Nd:YAG laser welding , 2002 .

[20]  A. Matsunawa Problems and solutions in deep penetration laser welding , 2001 .

[21]  J. Kenny,et al.  Development of high nitrogen, low nickel, 18%Cr austenitic stainless steels , 2000 .

[22]  H. D. Carlton,et al.  The Effect of Ar and N 2 Shielding Gas on Laser Weld Porosity in Steel , Stainless Steels , and Nickel , 2015 .