Aging of electrochemical double layer capacitors with acetonitrile-based electrolyte at elevated voltages

Abstract Laboratory-scale electrochemical capacitor cells with bound activated carbon electrodes and acetonitrile-based electrolyte were aged at various elevated constant cell voltages between 2.75 V and 4.0 V. During the constant voltage tests, the cell capacitance as well as the capacitance and resistance of each electrode was determined. Following each aging experiment, the cells were analyzed by means of electrochemical impedance spectroscopy, and the individual electrodes were characterized by gas adsorption and X-ray photoelectron spectroscopy. At cell voltages above 3.0 V, the positive electrode ages much faster than the negative. Both the capacitance loss and resistance increase of the cell could be totally attributed to the positive electrode. At cell voltages above 3.5 V also the negative electrode aged significantly. X-ray photoelectron spectroscopy indicated the presence of degradation products on the electrode surface with a much thicker layer on the positive electrode. Simultaneously, a significant decrease in electrode porosity could be detected by gas adsorption.

[1]  P. Lacaze,et al.  Electrochemical formation of thin polyacetonitrile films on a Pt surface , 1979 .

[2]  R. Kötz,et al.  Principles and applications of electrochemical capacitors , 2000 .

[3]  Dominique Massiot,et al.  Causes of supercapacitors ageing in organic electrolyte , 2007 .

[4]  P. Kurzweil,et al.  Electrochemical stability of organic electrolytes in supercapacitors: Spectroscopy and gas analysis of decomposition products , 2008 .

[5]  Philippe Azaïs Recherche des causes du vieillissement de supercondensateurs à électrolyte organique à base de carbones activés , 2003 .

[6]  R. Nozu,et al.  Investigation of the life process of the electric double layer capacitor during float charging , 2009 .

[7]  U. Starke,et al.  Chemical and electrochemical ageing of carbon materials used in supercapacitor electrodes , 2008 .

[8]  A. Wokaun,et al.  On the use of activated carbon as a quasi-reference electrode in non-aqueous electrolyte solutions , 2009 .

[9]  A. Burke Ultracapacitors: why, how, and where is the technology , 2000 .

[10]  R. Gallay,et al.  Pressure evolution in propylene carbonate based electrochemical double layer capacitors , 2006 .

[11]  R. Gallay,et al.  Comparison of pressure evolution in supercapacitor devices using different aprotic solvents , 2008 .

[12]  Takeshi Morimoto,et al.  Electric double-layer capacitor using organic electrolyte , 1996 .

[13]  R. Gallay,et al.  Interfacial Capacitance and Electronic Conductance of Activated Carbon Double-Layer Electrodes , 2004 .

[14]  Alexander Wokaun,et al.  Electrochemical characterization of single-walled carbon nanotubes for electrochemical double layer capacitors using non-aqueous electrolyte , 2009 .

[15]  A. Burke R&D considerations for the performance and application of electrochemical capacitors , 2007 .

[16]  Petr Novák,et al.  Gas evolution in activated carbon/propylene carbonate based double-layer capacitors , 2005 .

[17]  Yuichiro Asakawa,et al.  Degradation Responses of Activated-Carbon-Based EDLCs for Higher Voltage Operation and Their Factors , 2009 .

[18]  Y. Gogotsi,et al.  Materials for electrochemical capacitors. , 2008, Nature materials.

[19]  Dirk Uwe Sauer,et al.  Ageing behaviour of electrochemical double layer capacitors. Part I. Experimental study and ageing model , 2007 .

[20]  R. Kötz,et al.  Temperature behavior and impedance fundamentals of supercapacitors , 2006 .

[21]  V. Suryanarayanan,et al.  Electrochemical behavior of carbon electrodes in organic liquid electrolytes containing tetrafluoroborate and hexafluorophosphate anionic species in different non-aqueous solvent systems , 2005 .

[22]  B. Conway Electrochemical Supercapacitors: Scientific Fundamentals and Technological Applications , 1999 .

[23]  P. Biensan,et al.  Surface film formation on a carbonaceous electrode: Influence of the binder chemistry , 2009 .

[24]  J. Vetter,et al.  In situ atomic force microscopy study of dimensional changes during Li + ion intercalation/de-intercalation in highly oriented pyrolytic graphite , 2005 .

[25]  S. Biniak,et al.  The characterization of activated carbons with oxygen and nitrogen surface groups , 1997 .

[26]  R. Chambers,et al.  Surface Defluorination of PTFE by Sodium Atoms , 1994 .

[27]  Rémi Dedryvère,et al.  Surface film formation on a graphite electrode in Li‐ion batteries: AFM and XPS study , 2005 .

[28]  Alexander Wokaun,et al.  A comparison of the aging of electrochemical double layer capacitors with acetonitrile and propylene carbonate-based electrolytes at elevated voltages , 2010 .

[29]  H. Estrade-szwarckopf,et al.  U.P.S. and X.P.S. studies of alkali-graphite intercalation compounds , 1988 .

[30]  L. Kavan,et al.  Oxidation of Acetonitrile‐Based Electrolyte Solutions at High Potentials An In Situ Fourier Transform Infrared Spectroscopy Study , 1993 .

[31]  R. Gallay,et al.  Carbon based double layer capacitors with aprotic electrolyte solutions: the possible role of intercalation/insertion processes , 2006 .

[32]  B. Schmitt,et al.  In situ X-ray diffraction of the intercalation of (C2H5)4N+ and BF4- into graphite from acetonitrile and propylene carbonate based supercapacitor electrolytes , 2007 .

[33]  K. Beccu,et al.  Abschätzung der porenstruktur poröser elektroden aus impedanzmessungen , 1976 .