High temperature reactivity of two chromium-containing alloys in impure helium
暂无分享,去创建一个
Krzysztof Wolski | Gouenou Girardin | Céline Cabet | Fabien Rouillard | D. Kaczorowski | Michèle Pijolat | G. Girardin | M. Pijolat | K. Wolski | F. Rouillard | C. Cabet | J. Chapovaloff | D. Kaczorowski | J. Chapovaloff
[1] R. H. Cook. Creep Properties of lnconel-617 in Air and Helium at 800 to 1000°C , 1984 .
[2] Y. Kondo,et al. Kinetic studies of the reaction between Cr23 C6 particles and Cr2O3 particles , 1973 .
[3] H. McCoy,et al. Hastelloy-X for high-temperature gas-cooled reactor applications , 1984 .
[4] Willem J. Quadakkers,et al. Corrosion of High Temperature Alloys in the Primary Circuit Helium of High Temperature Gas Cooled Reactors. Part II: Experimental Results , 1985 .
[5] Willem J. Quadakkers,et al. Corrosion of high temprature alloys in the primary circuit helium of high temperature gas cooled reactors. – Part I: Theoretical background , 1985 .
[6] T. Nakanishi,et al. Creep Properties of Hastelloy-X in Impure Helium Environments , 1984 .
[7] Michel Lecomte,et al. ANTARES: The HTR/VHTR project at Framatome ANP , 2006 .
[8] H. Christ,et al. High temperature corrosion of the nickel-based alloy Inconel 617 in helium containing small amounts of impurities , 1987 .
[9] M. Tabarant,et al. High temperature corrosion of a nickel base alloy by helium impurities , 2007 .
[10] L. W. Graham,et al. The Development and Application of a Unified Corrosion Model for High-Temperature Gas-Cooled Reactor Systems , 1984 .
[11] M. R. Warren. Rapid decarburization and carburization in high temperature alloys in impure helium environments , 1986 .