Thermal cycling behavior and oxidation resistance of SiC whisker-toughened-mullite/SiC coated carbon/carbon composites in burner rig tests

[1]  H. Wadley,et al.  Fracture mechanisms of ytterbium monosilicate environmental barrier coatings during cyclic thermal exposure , 2016 .

[2]  Hejun Li,et al.  Microstructure and oxidation behavior of C/C–ZrB2–SiC composites coated with SiC coating at high temperature , 2015 .

[3]  Yu Xiaoyu,et al.  Microstructure and oxidation behavior of sol–gel mullite coating on SiC-coated carbon/carbon composites , 2015 .

[4]  Hejun Li,et al.  Effect of carbon nanotubes on the toughness, bonding strength and thermal shock resistance of SiC coating for C/C–ZrC–SiC composites , 2015 .

[5]  Hejun Li,et al.  A SiC-ZrB2-ZrC coating toughened by electrophoretically-deposited SiC nanowires to protect C/C composites against thermal shock and oxidation , 2015 .

[6]  Hejun Li,et al.  Oxidation protection of carbon/carbon composites by a novel SiC nanoribbon-reinforced SiC–Si ceramic coating , 2015 .

[7]  Hejun Li,et al.  Effect of pre-oxidation on the ablation resistance of ZrB2–SiC coating for SiC-coated carbon/carbon composites , 2015 .

[8]  Hejun Li,et al.  HfC nanowire-toughened TaSi2–TaC–SiC–Si multiphase coating for C/C composites against oxidation , 2015 .

[9]  Lai-fei Cheng,et al.  Strength and toughness improvement in a C/SiC composite reinforced with slurry-prone SiC whiskers , 2014 .

[10]  Hejun Li,et al.  Ablation behavior of Y2SiO5/SiC coating for C/C composites under oxyacetylene torch , 2014 .

[11]  Hejun Li,et al.  TaxHf1−xB2–SiC multiphase oxidation protective coating for SiC-coated carbon/carbon composites , 2014 .

[12]  Hejun Li,et al.  Oxidation protection of C/C composites with in situ bamboo-shaped SiC nanowire-toughened Si–Cr coating , 2013 .

[13]  Xiaohong Shi,et al.  Multilayer and multi-component oxidation protective coating system for carbon/carbon composites from room temperature to 1873 K , 2013 .

[14]  Hejun Li,et al.  Bamboo-shaped SiC nanowire-toughened SiC coating for oxidation protection of C/C composites , 2013 .

[15]  X. Xiong,et al.  SiC/SiC–YAG–YSZ oxidation protective coatings for carbon/carbon composites , 2013 .

[16]  Jianfeng Huang,et al.  A mullite/SiC oxidation protective coating for carbon/carbon composites , 2013 .

[17]  Yumin Zhang,et al.  Fabrication and characterization of SiC whisker reinforced reaction bonded SiC composite , 2013 .

[18]  Xiaohong Shi,et al.  Sealing role of B2O3 in MoSi2–CrSi2–Si/B-modified SiC coating for C/C composites , 2012 .

[19]  Q. Song,et al.  Improving the oxidation resistance of carbon/carbon composites at low temperature by controlling the grafting morphology of carbon nanotubes on carbon fibres , 2012 .

[20]  Hejun Li,et al.  High-temperature erosion resistance and aerodynamic oxidation mechanism of multi-layer MoSi2–CrSi2–Si/SiC coated carbon/carbon composites in a wind tunnel at 1873 K , 2012 .

[21]  Hejun Li,et al.  A SiC/ZrB2–SiC/SiC oxidation resistance multilayer coating for carbon/carbon composites , 2012 .

[22]  Hejun Li,et al.  Oxidation protection of SiC-coated C/C composites by SiC nanowire-toughened CrSi2–SiC–Si coating , 2012 .

[23]  Hejun Li,et al.  C/SiC/MoSi2–Si multilayer coatings for carbon/carbon composites for protection against oxidation , 2011 .

[24]  F. Béclin,et al.  Fabrication and characterization of composite sol–gel coatings on porous ceramic substrate , 2011 .

[25]  Hejun Li,et al.  Oxidation protection of C/SiC coated carbon/carbon composites with Si–Mo coating at high temperature , 2011 .

[26]  Hejun Li,et al.  Microstructure and oxidation of multi-layer MoSi2–CrSi2–Si coatings for SiC coated carbon/carbon composites , 2010 .

[27]  D. Sciti,et al.  Toughened ZrB2-based ceramics through SiC whisker or SiC chopped fiber additions , 2010 .

[28]  Hejun Li,et al.  SiC nanowire-toughened MoSi2–SiC coating to protect carbon/carbon composites against oxidation , 2010 .

[29]  Li Kezhi,et al.  A SiC whisker-toughened SiC-CrSi2 oxidation protective coating for carbon/carbon composites , 2007 .

[30]  G. Borchardt,et al.  Oxidation protection of C/C–SiC composites by an electrophoretically deposited mullite precursor: Cyclic thermogravimetric analysis , 2007 .

[31]  Xiaohong Shi,et al.  A MoSi2–SiC–Si/glass oxidation protective coating for carbon/carbon composites , 2006 .

[32]  Li Kezhi,et al.  SiC whisker-toughened MoSi2–SiC–Si coating to protect carbon/carbon composites against oxidation , 2006 .

[33]  Zhiyu Wang,et al.  In situ synthesis of super-long Cu nanowires inside carbon nanotubes with coal as carbon source , 2006 .

[34]  Donald M. Curry,et al.  Oxidation microstructure studies of reinforced carbon/carbon , 2006 .

[35]  P. Fauchais,et al.  Relationships between microstructure and electrical properties of RF and DC plasma-sprayed titania coatings , 2006 .

[36]  Xiaohong Shi,et al.  SiC whisker-toughened SiC oxidation protective coating for carbon/carbon composites , 2006 .

[37]  E. Boccaleri,et al.  A fast effective route to pH-dependent water-dispersion of oxidized single-walled carbon nanotubes , 2006 .

[38]  Stephan Schmidt,et al.  Advanced ceramic matrix composite materials for current and future propulsion technology applications , 2004 .

[39]  Narottam P. Bansal,et al.  Upper Temperature Limit of Environmental Barrier Coatings Based on Mullite and BSAS , 2003 .

[40]  T. Coyle,et al.  Temperature dependence of crack wake bridging stresses in a SiC-whisker-reinforced alumina , 2001 .

[41]  G. Borchardt,et al.  Mullite Based Oxidation Protection for SiC-C/C Composites in Air at Temperatures up to 1900 K , 1997 .

[42]  Chun-Hway Hsueh,et al.  Debonding of interfaces between beta-silicon nitride whiskers and SiAlY oxynitride glasses , 1996 .

[43]  N. Jacobson,et al.  New generation of plasma-sprayed mullite coatings on silicon carbide , 1995 .

[44]  Chun-Hway Hsueh,et al.  Toughening Behavior in Whisker‐Reinforced Ceramic Matrix Composites , 1988 .

[45]  A. Evans,et al.  On the toughening of ceramics by strong reinforcements , 1986 .