Verification of creep properties and rupture lifetime evaluation methods using small diameter Sn-3.0Ag-0.5Cu/Sn-58Bi/Sn-5Sb specimens

[1]  M. Gorley,et al.  Small punch creep investigation of Eurofer97 and 14Cr oxide dispersion strengthened steel , 2021, Nuclear Materials and Energy.

[2]  M. Sakane,et al.  Creep damage evaluation via uniaxial miniature testing for multiaxially stressed Mod.9Cr–1Mo steel components , 2021 .

[3]  A. Ballal,et al.  Evaluation of tensile properties of various regions of creep exposed dissimilar weld joint using miniature specimen testing , 2020 .

[4]  H. Wan,et al.  Small punch creep performance of heterogeneous microstructure dominated Inconel 718 fabricated by selective laser melting , 2020 .

[5]  M. Sakane,et al.  Development of miniature cruciform specimen and testing machine for multiaxial creep investigation , 2020 .

[6]  N. Pizúrová,et al.  Tensile, creep and fracture testing of prospective Fe-Al-based alloys using miniature specimens , 2019, Theoretical and Applied Fracture Mechanics.

[7]  M. Sakane,et al.  Effect of additional elements on the low-cycle-fatigue characteristics of Sn-1.0Ag-0.7Cu solder obtained using a miniature-sized specimen , 2018, International Journal of Fatigue.

[8]  X. Ling,et al.  Creep characteristics and deformation analysis of service-exposed material using small punch creep test , 2018 .

[9]  Fu-Zhen Xuan,et al.  Creep behavior of subzones in a CrMoV weldment characterized by the in-situ creep test with miniature specimens , 2018 .

[10]  Naveena,et al.  Effect of specimen size on small punch creep behavior of high nitrogen ferritic heat-resistant steels , 2018 .

[11]  文男 小川,et al.  非比例負荷におけるSn-8Zn-3Biはんだの多軸低サイクル疲労寿命 , 2017 .

[12]  Takamoto Itoh,et al.  Effect of Specimen Size and Oxygen Partial Pressure on Creep Characteristics for Mod. 9Cr-1Mo Steel , 2017 .

[13]  H. Hokazono,et al.  Effect of Additive Elements on Crack Initiation and Propagation Behavior at Stress Concentration Part for Sn-58Bi Solders , 2017 .

[14]  N. Hiyoshi High Temperature Tensile Strength Evaluation with Non-contact Measuring Method for Small Diameter Solders Specimen , 2016 .

[15]  N. Hiyoshi Creep-fatigue life evaluation of Sn-3.5Ag lead-free solder at low temperatures , 2016 .

[16]  雅健 旭吉 軸引張圧縮負荷によるSn-3.0Ag-0.5Cuの熱機械疲労寿命評価 , 2016 .

[17]  R. Lancaster,et al.  Elevated temperature creep deformation of a single crystal superalloy through the small punch creep method , 2015 .

[18]  Chao Wang,et al.  Low-cycle fatigue failure behavior and life evaluation of lead-free solder joint under high temperature , 2014, Microelectron. Reliab..

[19]  C. Suárez,et al.  Estimation of the mechanical properties of metallic materials by means of the small punch test , 2014 .

[20]  Y. Kariya,et al.  Effect of Temperature and Strain Rate on Low-Cycle Fatigue Life of Bi-Sn Eutectic Alloy , 2013 .

[21]  賢哉 河野,et al.  高温保持後のSn-3.0Ag-0.5Cuはんだ接合部の疲労寿命評価 , 2012 .

[22]  K. Yoon,et al.  Assessment of tensile strength using small punch test for transversely isotropic aluminum 2024 alloy produced by equal channel angular pressing , 2010 .

[23]  A. Kohyama,et al.  High-temperature strength analysis of welded joint of RAFs by small punch test , 2009 .

[24]  W. J. Plumbridge,et al.  Solders in electronics , 1996, Journal of Materials Science.

[25]  Hideaki Takahashi,et al.  Development of a further-miniaturized specimen of 3 mm diameter for tem disk (ø 3 mm) small punch tests , 1987 .

[26]  O. Buck,et al.  Evaluation of the ductile-to-brittle transition temperature shift due to temper embrittlement and neutron irradiation by means of a small-punch test , 1986 .