Magnetic properties of powder hard magnetic Fe–27Cr–10Co–0.5Mo and Fe–27Cr–10Co–2Mo alloys
暂无分享,去创建一个
Magnetic hysteresis properties of powder hard magnetic Fe–27Cr–10Co alloys with 0.5 and 2.0 wt % molybdenum were studied. For Fe–27Cr–10Co–0.5Mo alloy: Br = 1.35 T, HcB = 45.6 kA/m and (BH)max = 41 kJ/m3. For Fe–27Cr–10Co–2Mo alloy: Br = 1.29 T, HcB = 41 kA/m, (BH)max = 34.8 kJ/m3. It was shown that an alloying with 2 wt. % molybdenum of the low-cobalt powder hard magnetic Fe–27Cr–10Co alloy unlike high-cobalt hard magnetic FeCrCo alloys did not increase its magnetic hysteresis properties, reduced the camber of a demagnetization curve in a second quadrant.