Experimental Study on Fire Resistance of Building Steel Structure Fireproofing Material

The definition and connotation of the steel structure fire protection material are briefly given, and the relationship between the fire resistance and the HP/A is analyzed and summarized according to the domestic refractory test data of the typical laboratory exposed steel structure. According to the existing specification, the necessity of fireproof protection, the application and basic requirements of the steel structure fire protection material and the necessity of adopting the steel structure fire protection material are put forward, pointing out the existing problems of fire protection technology, exploring other fire protection materials. Reasonable proposal have been given for the fire resistance test standard system, the relevant standards and norms of the system: Develop different fire resistance test methods should be made for different fire situations, and the corresponding assessment methods should be made for practical engineering application. And then the further content that needs to be studied in this field has been pointed out. Although there are many deficiencies that the steel structure fire protection materials transfers from the development, product characteristics, test methods or standard systems and test data to the actual application of the transition, but the actual demand decisions the broad prospects of this area, so it is of great significance to carry out its fire performance test.

[1]  L. Berglund,et al.  Clay nanopaper as multifunctional brick and mortar fire protection coating—Wood case study , 2016 .

[2]  Emidio Nigro,et al.  Tests on intumescent paints for fire protection of existing steel structures , 2016 .

[3]  Guanglin Yuan,et al.  Quantitative risk assessment methods of evacuation safety for collapse of large steel structure gymnasium caused by localized fire , 2016 .

[4]  Yong Wang,et al.  Predicting intumescent coating protected steel temperature in fire using constant thermal conductivity , 2016 .

[5]  D. Peña,et al.  Role of Corrosion Products by the Sulfidation of Aisi/sae-1020 Steel in Heavy Crude Oil at High Temperatures , 2017 .

[6]  Sonia Giovinazzi,et al.  A group-AHP decision analysis for the selection of applied fire protection to steel structures , 2016 .

[7]  S. Bourbigot,et al.  Hydrocarbon time–temperature curve under airjet perturbation: An in situ method to probe char stability and integrity in reactive fire protection coatings , 2016 .

[8]  Fan Shenggang,et al.  Fire resistance of stainless steel beams with rectangular hollow section: Numerical investigation and design , 2016 .

[9]  New Pyrazine Derivatives as Efficient Inhibitors on Mild Steel Corrosion in Hydrochloric Medium , 2016 .

[10]  A. Mouritz,et al.  Multi-layer polymer metal laminates for the fire protection of lightweight structures , 2016 .

[12]  D. Peña,et al.  Influence of Temperature and Time on the Corrosion by Sulfidation of Aisi-316 Steel Exposed Under Transfer Line , 2017 .