High-temperature mechanical behaviour of flaw tolerant alumina–zirconia multilayered ceramics
暂无分享,去创建一个
[1] A. Sanchez-Herencia,et al. Processing optimisation and fracture behaviour of layered ceramic composites with highly compressive layers , 2007 .
[2] C. Baudín,et al. Flaw Tolerant Ceramic Laminates with Negligible Residual Stresses between Layers , 2007 .
[3] A. Sanchez-Herencia,et al. Residual stresses, strength and toughness of laminates with different layer thickness ratios , 2006 .
[4] R. Cook. Toughening of a Cordierite Glass–Ceramic by Compressive Surface Layers , 2005 .
[5] V. Sglavo,et al. Tailored Residual Stresses in High Reliability Alumina‐Mullite Ceramic Laminates , 2005 .
[6] R. Bermejo,et al. Thermal Shock Behavior of an Al2O3/ZrO2 Multilayered Ceramic with Residual Stresses due to Phase Transformations , 2005 .
[7] F. Lange,et al. Crack Bifurcation at the Surface of Laminar Ceramics That Exhibit a Threshold Strength , 2005 .
[8] E. Rybacki,et al. Mechanical and microstructural characterization of calcium aluminosilicate (CAS) and SiO2/CAS composites deformed at high temperature and high pressure , 2005 .
[9] C. Baudín,et al. Design and processing of Al2O3–Al2TiO5 layered structures , 2005 .
[10] A. Sanchez-Herencia,et al. Microstructure and High‐Temperature Mechanical Behavior of Alumina/Alumina–Yttria‐Stabilized Tetragonal Zirconia Multilayer Composites , 2005 .
[11] M. Lewis,et al. Apparent fracture toughness of Si3N4-based laminates with residual compressive or tensile stresses in surface layers , 2005 .
[12] F. Lange,et al. ZrO2/ZrO2 Layered Composites for Crack Bifurcation , 2004 .
[13] Guo‐Jun Zhang,et al. High-Temperature Multilayer Composites with Superplastic Interlayers , 2004 .
[14] J. Halloran,et al. Elevated‐Temperature Mechanical Properties of Silicon Nitride/Boron Nitride Fibrous Monolithic Ceramics , 2004 .
[15] N. Orlovskaya,et al. Crack arrest in Si3N4-based layered composites with residual stress , 2004 .
[16] Desiderio Kovar,et al. High-temperature deformation of Al2O3/Y-TZP particulate laminates , 2004 .
[17] G. Tan,et al. Effect of porous interlayers on crack deflection in ceramic laminates , 2004 .
[18] B. Sheldon,et al. A Layered Alumina Composite Tested at High Temperature in Air , 2000 .
[19] A. Domínguez-Rodríguez,et al. Effect of layer interfaces on the high-temperature mechanical properties of alumina/zirconia laminate composites , 2000 .
[20] F. Lange,et al. Bifurcation in alumina plates produced by a phase transformation in central, alumina/zirconia thin layers , 2000 .
[21] Yang,et al. Direct adjustment procedure for weight functions of graded materials , 2000 .
[22] D. Munz,et al. Applicability of the extended Petroski–Achenbach weight function procedure to graded materials , 2000 .
[23] Rao,et al. Laminar Ceramics That Exhibit a Threshold Strength. , 1999, Science.
[24] Green,et al. Crack Arrest and Multiple Cracking in Glass Through the Use of Designed Residual Stress Profiles. , 1999, Science.
[25] E. Roncari,et al. High temperature plastic deformation of multilayered YTZP/ZTA composites obtained by tape casting , 1998 .
[26] W. Clegg. Design of ceramic laminates for structural applications , 1998 .
[27] B. Bollen,et al. Impulse excitation apparatus to measure resonant frequencies, elastic moduli, and internal friction at room and high temperature , 1997 .
[28] H. M. Chan. LAYERED CERAMICS: Processing and Mechanical Behavior , 1997 .
[29] M. Oechsner,et al. Crack Bifurcation in Laminar Ceramic Composites , 1996 .
[30] A. Evans,et al. Crack deflection at an interface between dissimilar elastic materials: Role of residual stresses , 1994 .
[31] Linghui He,et al. A linear theory of laminated shells accounting for continuity of displacements and transverse shear stresses at layer interfaces , 1994 .
[32] J. E. Ritter,et al. Erosion damage and strength degradation of zirconia-toughened alumina , 1988 .
[33] B. Lawn,et al. A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: II, Strength Method , 1981 .
[34] S. Timoshenko,et al. Theory of elasticity , 1975 .
[35] J. Dundurs. Discussion: ``Edge-Bonded Dissimilar Orthogonal Elastic Wedges Under Normal and Shear Loading'' (Bogy, D. B., 1968, ASME J. Appl. Mech., 35, pp. 460-466) , 1969 .
[36] C. Smith,et al. Calculated High‐Temperature Elastic Constants for Zero Porosity Monoclinic Zirconia , 1964 .
[37] J. B. Wachtman,et al. Young's Modulus of Various Refractory Materials as a Function of Temperature , 1959 .
[38] A. Sanchez-Herencia,et al. Threshold strength evaluation on an Al2O3–ZrO2 multilayered system , 2007 .
[39] J. Gurauskis,et al. Alumina–zirconia layered ceramics fabricated by stacking water processed green ceramic tapes , 2007 .
[40] G. D. Portu,et al. Effective fracture toughness in Al2O3–Al2O3/ZrO2 laminates , 2007 .
[41] C. Baudín,et al. Layered materials with high strength and flaw tolerance based on alumina and aluminium titanate , 2007 .
[42] R. Danzer,et al. Prediction of the fracture toughness of a ceramic multilayer composite – Modeling and experiments , 2007 .
[43] A. Sanchez-Herencia,et al. Fracture behaviour of an Al2O3-ZrO2 multi-layered ceramic with residual stresses due to phase transformations , 2006 .
[44] Rolf W. Steinbrech,et al. Mechanical properties of coated materials and multi-layered composites determined using bending methods , 2004 .
[45] Theo Fett,et al. Stress intensity factors and weight functions , 1997 .
[46] Z. Suo,et al. Mixed mode cracking in layered materials , 1991 .
[47] John W. Hutchinson,et al. Crack deflection at an interface between dissimilar elastic-materials , 1989 .
[48] J. Srawley. Wide range stress intensity factor expressions for ASTM E 399 standard fracture toughness specimens , 1976, International Journal of Fracture.
[49] J. Dundurs,et al. Discussion of Edge-Bonded Dissimilar Orthogonal Elastic Wedges under Normal and Shear Loading , 1969 .