Optimization of the sintering atmosphere for high-density hydroxyapatite–carbon nanotube composites

Hydroxyapatite–carbon nanotube (HA–CNT) composites have the potential for improved mechanical properties over HA for use in bone graft applications. Finding an appropriate sintering atmosphere for this composite presents a dilemma, as HA requires water in the sintering atmosphere to remain phase pure and well hydroxylated, yet CNTs oxidize at the high temperatures required for sintering. The purpose of this study was to optimize the atmosphere for sintering these composites. While the reaction between carbon and water to form carbon monoxide and hydrogen at high temperatures (known as the ‘water–gas reaction’) would seem to present a problem for sintering these composites, Le Chatelier's principle suggests this reaction can be suppressed by increasing the concentration of carbon monoxide and hydrogen relative to the concentration of carbon and water, so as to retain the CNTs and keep the HA's structure intact. Eight sintering atmospheres were investigated, including standard atmospheres (such as air and wet Ar), as well as atmospheres based on the water–gas reaction. It was found that sintering in an atmosphere of carbon monoxide and hydrogen, with a small amount of water added, resulted in an optimal combination of phase purity, hydroxylation, CNT retention and density.

[1]  S. Dorozhkin Calcium Orthophosphates in Nature, Biology and Medicine , 2009, Materials.

[2]  Khiam Aik Khor,et al.  Preparation and characterization of a novel hydroxyapatite/carbon nanotubes composite and its interaction with osteoblast-like cells , 2009 .

[3]  C. Tsui,et al.  Fabrication and characterization of needle-like nano-HA and HA/MWNT composites , 2008, Journal of materials science. Materials in medicine.

[4]  K. Sun,et al.  Mechanical properties, microstructure and histocompatibility of MWCNTs/HAp biocomposites , 2007 .

[5]  Ashley A. White,et al.  Hydroxyapatite–Carbon Nanotube Composites for Biomedical Applications: A Review , 2007 .

[6]  Besim Ben-Nissan,et al.  Development of carbon nanotube-reinforced hydroxyapatite bioceramics , 2006 .

[7]  M. Nygren,et al.  Spark Plasma Sintering: Possibilities and Limitations , 2004 .

[8]  A. Dorner-Reisel,et al.  Thermogravimetric and thermokinetic investigation of the dehydroxylation of a hydroxyapatite powder , 2004 .

[9]  Lian Gao,et al.  Novel in situ synthesis of MWNTs-hydroxyapatite composites , 2004 .

[10]  A. Peigney Tougher ceramics with nanotubes , 2003, Nature materials.

[11]  F. Lin,et al.  Thermal decomposition and reconstitution of hydroxyapatite in air atmosphere. , 1999, Biomaterials.

[12]  L. Yubao,et al.  Relationship between the colour change of hydroxyapatite and the trace element manganese. , 1993, Biomaterials.

[13]  T. Chaki,et al.  Sintering behaviour and mechanical properties of hydroxyapatite and dicalcium phosphate , 1993 .

[14]  Larry L. Hench,et al.  Bioceramics: From Concept to Clinic , 1991 .

[15]  C. Klein,et al.  Studies of the solubility of different calcium phosphate ceramic particles in vitro. , 1990, Biomaterials.

[16]  E. Keller,et al.  Iliac bone grafting: review of 160 consecutive cases. , 1987, Journal of oral and maxillofacial surgery : official journal of the American Association of Oral and Maxillofacial Surgeons.

[17]  J. Trombe,et al.  Some features of the incorporation of oxygen in different oxidation states in the apatitic lattice—I On the existence of calcium and strontium oxyapatites , 1978 .