Self-lubricating composites containing MoS2: A review

Abstract Consistent and concise literature about self-lubricating metallic composites containing MoS2 is very scarce in particular those analyzing the possible reactions during processing, which are often neglected or even unknown in a variety of publications. In some situations, the composites present a poor lubricating behavior not related to environmental parameters or surface properties, but due to the simple fact that the solid lubricant added is not there anymore, i.e. it has reacted with the matrix or other additives. This review compiled publications from 1945 up to 2017 about the research developments in metal matrix self-lubricating composites containing MoS2. Information on the tribological properties of such composites according to the varied matrixes, contents, processing conditions, testing temperatures and atmospheres are presented.

[1]  A. K. Pogosian,et al.  Friction and wear studies using Taguchi method on polyphenylene sulfide filled with a complex mixture of MoS2, Al2O3, and other compounds , 2005 .

[2]  D. Xiong,et al.  Friction and wear properties of Ni–Cr–W–Al–Ti–MoS2 at elevated temperatures and self-consumption phenomena , 2008 .

[3]  B. Tatarchuk,et al.  Surface and buried-interfacial reactivity of iron and MoS2: a study of laser-deposited materials , 1996 .

[4]  J. Bressan,et al.  Study of wear in self-lubricating composites for application in seals of electric motors , 2006 .

[5]  S. Danyluk,et al.  The tribological properties and mechanism of wear of Cu-based sintered powder materials containing molybdenum disulfide and molybdenum diselenite under unlubricated sliding against copper , 2012 .

[6]  J. Robertson Diamond-like amorphous carbon , 2002 .

[7]  Stefan Gheorghe,et al.  Development of New PM Iron-Based Materials for Self-Lubricating Bearings , 2011 .

[8]  S. Takayanagi,et al.  Friction and wear properties of lead-free aluminum alloy bearing material with molybdenum disulfide layer by a reciprocating test , 2013 .

[9]  Yafei Lu,et al.  A combinatorial approach for automotive friction materials: Effects of ingredients on friction performance , 2006 .

[10]  Yufu Xu,et al.  Tribological Properties of MoS2 with Different Morphologies in High-Density Polyethylene , 2012, Tribology Letters.

[11]  U. Tewari,et al.  Influence of fillers and fibre reinforcement on abrasive wear resistance of some polymeric composites , 1990 .

[12]  I. Negulescu,et al.  Sliding wear behavior of PTFE composites , 2002 .

[13]  Y. Liu,et al.  Tribological behaviour of silver based self-lubricating composite , 2013 .

[14]  M. Kosec,et al.  The influence of MoS2 additions on the densification of water-atomized HSS powders , 2006 .

[15]  Kenneth C. Ludema,et al.  Friction Wear Lubrication: A Textbook in Tribology , 1996 .

[16]  Wenzheng Zhai,et al.  Synergetic lubricating effect of MoS2 and Ti3SiC2 on tribological properties of NiAl matrix self-lubricating composites over a wide temperature range , 2014 .

[17]  J. Lin,et al.  Experimental analysis of the tribological behavior of electroless nickel-coated graphite particles in aluminum matrix composites under reciprocating motion , 2000 .

[18]  Farshad Akhlaghi,et al.  Influence of graphite content on the dry sliding and oil impregnated sliding wear behavior of Al 2024-graphite composites produced by in situ powder metallurgy method , 2009 .

[19]  N. I. Smirnov,et al.  Thermal-diffusion synthesis of thick molybdenum disulphide coatings on steel substrates , 2004 .

[20]  S. Dolinsek,et al.  The characteristics of vacuum sintered M3/2 type HSSs with MoS2 addition , 2003 .

[21]  Yufu Xu,et al.  Structural, thermal, and tribological properties of intercalated polyoxymethylene/molybdenum disulfide nanocomposites , 2008 .

[22]  Anna C. Domask,et al.  Transition Metal–MoS2 Reactions: Review and Thermodynamic Predictions , 2015, Journal of Electronic Materials.

[23]  D. Teer,et al.  The tribological properties of MoS2/metal composite coatings deposited by closed field magnetron sputtering , 1997 .

[24]  J. Craig,et al.  Mineral chemistry of metal sulfides , 1978 .

[25]  P. Taborek,et al.  Friction of molybdenum disulfide–titanium films under cryogenic vacuum conditions , 2011 .

[26]  A. G. Kostornov,et al.  Sintered antifriction materials , 1969 .

[27]  W. Xiao,et al.  Tribology performances of molybdenum disulfide reinforced thermoplastic polyimide under dry and water lubrication conditions , 2006 .

[28]  H. Shao,et al.  Friction and Wear Behaviors of Ag/MoS2/G Composite in Different Atmospheres and at Different Temperatures , 2012, Tribology Letters.

[29]  V. A. Shapovalov,et al.  Peculiarities of tribological behavior of low-filled composites based on polytetrafluoroethylene (PTFE) and molybdenum disulfide , 2014 .

[30]  S. K. Malhotra,et al.  Tribological characteristics of filled ultrahigh molecular weight high density polyethene , 1993 .

[31]  B. Gorman,et al.  Atomic Layer Deposition of Tungsten Disulphide Solid Lubricant Nanocomposite Coatings on Rolling Element Bearings , 2009 .

[32]  M. Xue High temperature oxidation and wear behaviour of powder metallurgically developed Ni-Cr-W-Al-Ti-MoS 2 composite , 2009 .

[33]  Hui-di Zhou,et al.  A comparative investigation of the friction and wear behavior of polyimide composites under dry sliding and water-lubricated condition , 2003 .

[34]  Hui-di Zhou,et al.  Preparation and properties of MoS2/a-C films for space tribology , 2013 .

[35]  B. Ramesh,et al.  Optimization of tribological parameters in abrasive wear mode of carbon-epoxy hybrid composites , 2014 .

[36]  I. Efeoglu,et al.  Tribological characteristics of MoS2–Nb solid lubricant film in different tribo-test conditions , 2008 .

[37]  S. Shil’ko,et al.  Wear resistance of composites based on ultrahigh molecular weight polyethylene filled with graphite and molybdenum disulfide microparticles , 2014 .

[38]  R. Tenne,et al.  Fullerene‐like WS2 Nanoparticles: Superior Lubricants for Harsh Conditions , 2003 .

[39]  Da-yung Wang,et al.  Microstructural and tribological characterization of MoS2-Ti composite solid lubricating films , 1999 .

[40]  N. Chen,et al.  A study of the optimization mechanism of solid lubricant concentration in self-lubricating composite , 1997 .

[41]  R. Oberacker,et al.  An introduction to powder metallurgy , 1993 .

[42]  A. Abdollah-zadeh,et al.  Microstructural and tribological properties of Al5083 based surface hybrid composite produced by friction stir processing , 2012 .

[43]  Siddaramaiah,et al.  Polycarbonate/molybdenum disulfide/carbon black composites: Physicomechanical, thermal, wear, and morphological properties , 2012 .

[44]  Ł. Wierzbicki,et al.  Tribological Properties of Copper-Based Composites with Lubricating Phase Particles , 2014 .

[45]  P. Skarvelis,et al.  Microstructural and tribological evaluation of potential self-lubricating coatings with MoS2⧹MnS additions produced by the plasma transferred arc technique , 2009 .

[46]  H. Assadi,et al.  Effect of applied load on the dry sliding wear behaviour and the subsurface deformation on hybrid metal matrix composite , 2013 .

[47]  A. Molinari,et al.  Dry sliding wear of ferrous PM materials , 2001 .

[48]  S. Dhanasekaran,et al.  Gear tooth wear in sintered spur gears under dry running conditions , 2008 .

[49]  M. Fazel,et al.  Effect of solid lubricant particles on room and elevated temperature tribological properties of Ni–SiC composite coating , 2014 .

[50]  Fernando Wypych Dissulfeto de molibdênio, um material multifuncional e surpreendente: doze anos depois , 2014 .

[51]  F. Bülbül,et al.  Effect of crystallographic orientation on the friction and wear properties of MoxSy-Ti coatings by pulsed-dc in nitrogen and humid air , 2005 .

[52]  K. Simha,et al.  Study of solid lubrication with MoS2 coating in the presence of additives using reciprocating ball-on-flat scratch tester , 2008 .

[53]  Yoshitada Watanabe Sliding contact characteristics between composite materials containing layered solid lubricants and carbon , 1992 .

[54]  T. Suhonen,et al.  Microstructure and tribological properties of pulsed electric current sintered alumina–zirconia nanocomposites with different solid lubricants , 2013 .

[55]  M. Gardos Self-lubricating composites for extreme environment applications , 1982 .

[56]  S. Raadnui,et al.  Tribological behaviour of sintered 316L stainless steel impregnated with MoS2 plain bearing , 2008 .

[57]  R. Gnanamoorthy,et al.  Dry sliding friction and wear characteristics of Fe–C–Cu alloy containing molybdenum di sulphide , 2007 .

[58]  Zafer Kazancı,et al.  Friction and wear behaviors of aircraft brake linings material , 2012 .

[59]  H. Meerkamm,et al.  A new type of tribological coating for machine elements based on carbon, molybdenum disulphide and titanium diboride , 2004 .

[60]  Hong Liang,et al.  Characterization and frictional behavior of nanostructured Ni–W–MoS2 composite coatings , 2009 .

[61]  Vasile Bratu,et al.  Tribological behaviour and statistical experimental design of sintered iron-copper based composites , 2013 .

[62]  J. Lee,et al.  Polyamide 6/carbon black/molybdenum disulphide composites: Friction, wear and morphological characteristics , 2013 .

[63]  S. Raadnui,et al.  Dry sliding wear behavior of SS316L composites containing h-BN and MoS2 solid lubricants , 2014 .

[64]  F. Yang,et al.  Sliding wear of epoxy compounds against different counterparts under dry and aqueous conditions , 2004 .

[65]  Wenzheng Zhai,et al.  Tribological behaviors of NiAl based self-lubricating composites containing different solid lubricants at elevated temperatures , 2014 .

[66]  S. Kim,et al.  Tribological properties of solid lubricants (graphite, Sb2S3, MoS2) for automotive brake friction materials , 2006 .

[67]  K. Furlan,et al.  Influence of alloying elements on the sintering thermodynamics, microstructure and properties of Fe–MoS2 composites , 2015 .

[68]  D. King,et al.  Atomic layer deposition of solid lubricating coatings on particles , 2012 .

[69]  Zhenguo Yang,et al.  Mechanical and tribological properties of polyoxymethylene modified with nanoparticles and solid lubricants , 2008 .

[70]  Jin-jun Lu,et al.  Tribological characteristics of electroless Ni-P-MoS2 composite coatings at elevated temperatures , 2013 .

[71]  A. Lansdown Molybdenum Disulphide Lubrication , 1999 .

[72]  D. C. Evans,et al.  Self-lubricating materials for plain bearings , 1982 .

[73]  A. Erdemir,et al.  Solid Lubricant Coatings: Recent Developments and Future Trends , 2004 .

[74]  R. Gnanamoorthy,et al.  Microstructure, strength and tribological behavior of Fe–C–Cu–Ni sintered steels prepared with MoS2 addition , 2007 .

[75]  T. Goto,et al.  Unbalanced magnetron sputtered Ti–Si–N:MoSx composite coatings for improvement of tribological properties , 2005 .

[76]  H. Wiśniewska-Weinert Experimental study and modelling of mixed particulate lubrication with MoS 2 powder solid lubricant , 2011 .

[77]  R. Gnanamoorthy,et al.  Abrasive wear behavior of sintered steels prepared with MoS2 addition , 2007 .

[78]  M.M.H. Megat Ahmad,et al.  A review on tribological performance of natural fibre polymeric composites , 2015 .

[79]  U. Tewari,et al.  Influence of solid lubricants and fibre reinforcement on wear behaviour of polyethersulphone , 2000 .

[80]  R. Tenne,et al.  New nanotechnology solid lubricants for superior dry lubrication , 2003 .

[81]  F. Zerbetto,et al.  Stability, dynamics, and lubrication of MoS2 platelets and nanotubes. , 2012, Langmuir : the ACS journal of surfaces and colloids.

[82]  U. Tewari,et al.  On the abrasive wear of some polyimides and their composites , 1991 .

[83]  M. Dugger,et al.  Atomic layer deposition of tungsten disulphide solid lubricant thin films , 2004 .

[84]  Xiong Dangsheng Lubrication behavior of Ni–Cr-based alloys containing MoS2 at high temperature , 2001 .

[85]  Tribological performance of MoS2B2O3 compacts , 1990 .

[86]  Stephen Robert Shatynski,et al.  The thermochemistry of transition metal sulfides , 1977 .

[87]  R. Tenne,et al.  Superior tribological properties of powder materials with solid lubricant nanoparticles , 2003 .

[88]  A. Erdemir Solid Lubricants and Self-Lubricating Films , 2001 .

[89]  V. Leskovšek,et al.  Vacuum sintering of water-atomised HSS powders with MoS2 additions , 2001 .

[90]  F. Yi,et al.  Structure and Formation Mechanism of Surface Film of Ag-MoS2 Composite during Electrical Sliding Wear , 2009 .

[91]  Jie Yao,et al.  Effect of Sliding Speed and Applied Load on Dry Sliding Tribological Performance of TiAl Matrix Self-lubricating Composites , 2014, Tribology Letters.

[92]  Yoshitada Watanabe High-speed sliding characteristics of Cu–Sn-based composite materials containing lamellar solid lubricants by contact resistance studies , 2008 .

[93]  Yi Feng,et al.  Friction and wear properties of Cu-based self-lubricating composites in air and vacuum conditions , 2012 .

[94]  D. Xiong,et al.  Tribological properties of nickel-based self-lubricating composite at elevated temperature and counterface material selection , 2008 .

[95]  Michel Jeandin,et al.  The role of porosity in the dry sliding wear of a sintered ferrous alloy , 1994 .

[96]  B. Wendler,et al.  Microstructure and tribological properties of low-friction composite MoS2(Ti,W) coating on the oxygen hardened Ti-6Al-4V alloy , 2014, Metals and Materials International.

[97]  Sintered iron-copper-tin-lead antifriction materials : effect of temperature , 2000 .

[98]  Gabriel A. Lima,et al.  Metallurgical Aspects of Self-lubricating Composites Containing Graphite and MoS2 , 2017, Journal of Materials Engineering and Performance.

[99]  S. H. Kim Influence of sulfides on the tribological properties of composites produced by pulse electric current sintering , 2014, International Journal of Minerals, Metallurgy, and Materials.

[100]  Yoshiro Iwai,et al.  Wear and mechanical properties of sintered copper-tin composites containing graphite or molybdenum disulfide , 2003 .

[101]  S. Mohney,et al.  Oxidation and oxidative vapor-phase etching of few-layer MoS2 , 2017 .

[102]  J. Farr Molybdenum disulphide in lubrication. A review , 1975 .