Pr1.33Pt4Ga10: Superstructure and Magnetism.

Pr1.33Pt4Ga10 single crystals are prepared from the elements using excess Ga as flux (alumina crucible in evacuated silica ampoule, 1150 °C, 4 h, 2; ≈10% yield).