Synthesis, microstructure and mechanical properties of (Mo,Ti)Si2/Al2O3 composites prepared by thermite-reaction-assisted combustion synthesis

[1]  Guo‐Jun Zhang,et al.  Pressureless sintering, mechanical properties and oxidation behavior of ZrB2 ceramics doped with B4C , 2015 .

[2]  Xiaohong Wang,et al.  Thermodynamic calculation and an experimental study of the combustion synthesis of (Mo1−xNbx)Si2 (0 ⩽ x ⩽ 1) , 2015 .

[3]  Xiaohong Wang,et al.  High-temperature crack-healing behaviour and strength recovery of (MoNb)Si2 , 2015 .

[4]  Xiaohong Wang,et al.  Effect of annealing environment on the crack healing and mechanical properties of (Mo0.97Nb0.03)(Si0.97Al0.03)2 , 2015 .

[5]  F. Akhtar,et al.  Synthesis, microstructure and properties of MoSi2–5 vol%Al2O3 composites , 2014 .

[6]  A. Abdollahi,et al.  Effect of B4C, MoSi2, nano SiC and micro-sized SiC on pressureless sintering behavior, room-temperature mechanical properties and fracture behavior of Zr(Hf)B2-based composites , 2014 .

[7]  V. Gorshkov,et al.  SHS Casting of (Mo,W)Si2, (Mo,Nb)Si2, and (Mo,Ti)Si2 silicides: effect of activating 3CaO2 + 2Al additives , 2014, International Journal of Self-Propagating High-Temperature Synthesis.

[8]  M. Razavi,et al.  The effect of temperature on the in situ synthesis–sintering and mechanical properties of MoSi2 prepared by spark plasma sintering , 2014 .

[9]  Du Lihui,et al.  OXIDATION BEHAVIOR OF IN SITU SYNTHESIZED MoSi2-SiC COMPOSITES AT 500 degrees C , 2013 .

[10]  Dezhi Wang,et al.  Preparation and characterization of sintered molybdenum doped with MoSi2/La2O3/Y2O3 composite particle , 2012 .

[11]  Q. Xue,et al.  Tribo-pair dependence of friction and wear moisture sensitivity for a-C:Si:Al carbon-based coating , 2012 .

[12]  Xiaohong Wang,et al.  Combustion synthesis of (Mo1 − xCrx)Si2 (x = 0.00–0.30) alloys in SHS mode , 2012 .

[13]  M. Vilasi,et al.  The oxidation behaviour of uniaxial hot pressed MoSi2 in air from 400 to 1400 °C , 2011 .

[14]  Xiaohong Wang,et al.  Effects of boron addition on the formation of MoSi2 by combustion synthesis mode , 2010 .

[15]  A. K. Suri,et al.  Thermal and electrical properties of TiB2–MoSi2 , 2010 .

[16]  J. Perepezko The Hotter the Engine, the Better , 2009, Science.

[17]  Houan Zhang,et al.  MoSi2 oxidation resistance coatings for Mo5Si3/MoSi2 composites , 2009 .

[18]  Yicheng Ge,et al.  Reactive Hot Pressing of SiC/MoSi2 Nanocomposites , 2007 .

[19]  Kun‐Lin Lin,et al.  Reaction Between Titanium and Zirconia Powders During Sintering at 1500°C , 2007 .

[20]  R. Mitra Mechanical behaviour and oxidation resistance of structural silicides , 2006 .

[21]  J. Lee,et al.  A study of tungsten nanopowder formation by self-propagating high-temperature synthesis , 2005 .

[22]  E. Ström,et al.  Processing, microstructure and properties of C40 Mo(Si,Al)2/Al2O3 composites , 2003 .

[23]  A. Heron,et al.  Mechanical alloying of MoSi2 with ternary alloying elements. Part 1: Experimental , 2003 .

[24]  J. Bowen,et al.  The effect of coarse second-phase particles on the rate of grain refinement during severe deformation processing , 2003 .

[25]  A. Umarji,et al.  Synthesis and structure of aluminum substituted MoSi2 , 2003 .

[26]  A. Shan,et al.  Phase transformation and indentation response in the surface of MoSi2 exposed to vacuum at high temperature , 2003 .

[27]  J. A. Sekhar,et al.  Microstructure and properties of MoSi2–MoB and MoSi2–Mo5Si3 molybdenum silicides , 2003 .

[28]  K. Hirota,et al.  Fabrication and mechanical properties of monolithic MoSi2 by spark plasma sintering , 2002 .

[29]  W. Fang,et al.  Effect of Mg addition on the microstructure and mechanical properties of MoSi2 alloys , 2002 .

[30]  T. Nakano,et al.  Microstructure of duplex-phase NbSi2(C40)/MoSi2(C11b) crystals containing a single set of lamellae , 2002 .

[31]  Y. Kimura,et al.  Microstructure and Phase Stability in MoSi2-TSi2 (T=Cr, V, Nb, Ta, Ti) Pseudo-Binary Systems. , 2001 .

[32]  T. Mitchell,et al.  Solid solution hardening and softening in MoSi2 alloys , 2001 .

[33]  Y. Park,et al.  Microstructure and Mechanical Properties of MoSi2/Nb Composites Made by MA-Pulse Discharge Sintering , 2000 .

[34]  J. Petrovic Toughening strategies for MoSi2-based high temperature structural silicides , 2000 .

[35]  Makoto Yoshida,et al.  Interfacial modification and impact properties of Nb/MoSi2 laminate composites by the addition of ZrO2, NbSi2, and SiC particles , 2000 .

[36]  K. Matsuura,et al.  Synthesis of MoSi2-TiSi2 pseudobinary alloys by reactive sintering , 2000 .

[37]  A. K. Vasudevan,et al.  Key developments in high temperature structural silicides , 1999 .

[38]  M. Kramer,et al.  Boron-doped molybdenum silicides for structural applications , 1999 .

[39]  H. Herman,et al.  Processing and properties of MoSi2–SiC and MoSi2–Al2O3 , 1999 .

[40]  Guo‐Jun Zhang,et al.  Addition effects of aluminum and in situ formation of alumina in MoSi2 , 1999 .

[41]  Yong-Seog Kim,et al.  On the formation of MoSi2 by self-propagating high-temperature synthesis , 1996 .

[42]  W. Boettinger,et al.  Application of ternary phase diagrams to the development of MoSi2-based materials , 1992 .

[43]  A. Vasudévan,et al.  A comparative overview of molybdenum disilicide composites , 1992 .

[44]  E. Hall,et al.  The Deformation and Ageing of Mild Steel: III Discussion of Results , 1951 .

[45]  张来启,et al.  原位合成 MoSi 2 -SiC复合材料在 500℃的氧化行为 , 2013 .

[46]  A. Johansson,et al.  Guiding of highly charged ions through insulating nanocapillaries , 2008 .

[47]  A. Shan,et al.  Tailoring the microstructure of molybdenum disilicide matrix composites with Nb additions , 2004 .

[48]  H. Inui,et al.  High-temperature structural intermetallics , 2000 .

[49]  K. Nagata,et al.  Effect of third elements on the pesting suppression of Mo-Si-X intermetallics (X = Al, Ta, Ti, Zr and Y) , 1996 .

[50]  V. M. Mal'tsev,et al.  Some principles of combustion of titanium-silicon mixtures , 1979 .

[51]  N. Petch,et al.  The Cleavage Strength of Polycrystals , 1953 .