Freeform fabrication of titanium metal by 3D micro welding

Abstract A novel freeform fabrication method named 3D micro welding (3DMW) has been developed. It is a combined process of the freeform fabrication method with TIG (tungsten inert gas) welding. The titanium micro beads were investigated with respect to the diameter, height, and contact angle to the titanium substrate as functions of arc discharge current and two different shielding gases. The Ar-4% H2 gas was more effective in preventing oxidization of beads than Ar gas. Simple 3D titanium objects with arch, arabic numerals and pyramidal shapes were formed. Fine needle-like solidification structure of α-phase titanium were developed during bead formation due to the rapid cooling of the melt. The interfaces between a titanium bead and titanium substrate were jointed well without cracks or pores.

[1]  Ernst-Wolfgang Kreutz,et al.  Rapid prototyping with CO2 laser radiation , 1995 .

[2]  Xue Yan,et al.  PII: 0010-4485(95)00035-6 , 2003 .

[3]  S. Emura,et al.  Blended elemental P/M synthesis and property evaluation of Ti-1100 alloy , 2003 .

[4]  Radovan Kovacevic,et al.  Droplet formation, detachment, and impingement on the molten pool in gas metal arc welding , 1999 .

[5]  Eui W. Lee,et al.  Correlation of fatigue properties and microstructure in investment cast Ti-6Al-4V welds , 2003 .

[6]  P. Fauchais,et al.  Plasma spraying: Present and future , 1994 .

[7]  G. K. Lewis,et al.  Direct Laser Metal Deposition Process Fabricates Near-Net-Shape Components Rapidly , 1995 .

[8]  S. E. Kim,et al.  Directional solidification of TiAl base alloys using a polycrystalline seed , 2002 .

[9]  Conor O'Mahony,et al.  Titanium as a micromechanical material , 2002 .

[10]  G. Liang,et al.  Pore formation during hybrid laser-tungsten inert gas arc welding of magnesium alloy AZ31B—mechanism and remedy , 2005 .

[11]  David L. Bourell,et al.  Direct laser freeform fabrication of high performance metal components , 1998 .

[12]  S. E. Kim,et al.  Mechanical and oxidation properties of Ti–xFe–ySi alloys , 2002 .

[13]  M. Hoffmann,et al.  Bulk silicon micromachining for MEMS in optical communication systems , 2002 .

[14]  Chun‐Sing Lee,et al.  Effects of microstructural parameters on the fatigue crack growth of fully lamellar γ-TiAl alloys , 2002 .

[15]  Bo-Sung Shin,et al.  Development of a direct metal freeform fabrication technique using CO2 laser welding and milling technology , 2001 .

[16]  R Kovacevic,et al.  Rapid prototyping based on variable polarity gas tungsten arc welding for a 5356 aluminium alloy , 2001 .

[17]  Nam P. Suh,et al.  Droplet-Based Manufacturing , 1993 .

[18]  Noshir A. Langrana,et al.  Structural quality of parts processed by fused deposition , 1996 .

[19]  Yiwei Chen,et al.  Automated system for welding-based rapid prototyping , 2002 .