General and Localized Corrosion of Outer Barrier of High-Level Waste Container in Yucca Mountain
暂无分享,去创建一个
John C. Estill | Joseph C. Farmer | D. McCright | G. E. Gdowski | F. Wang | T. Summers | P. J. Bedrossian | J. Horn | Tiangan Lian | A. Lingenfelter | W. G. Halsey
[1] G. Gdowski. Formulation and make-up of simulated acidic concentrated water (SAW), high ionic content aqueous solution , 1996 .
[2] G. E. Gdowski,et al. Survey of degradation modes of four nickel-chromium-molybdenum alloys , 1991 .
[3] W. M. Haynes. CRC Handbook of Chemistry and Physics , 1990 .
[4] R. D. McCright,et al. Engineered materials characterization report for the Yucca Mountain Site Characterization Project. Volume 2, Design data , 1995 .
[5] T Summers,et al. Aging and phase stability of waste package outer barrier , 1999 .
[6] G. G. Stokes. "J." , 1890, The New Yale Book of Quotations.
[7] R. D. McCright,et al. General Corrosion and Localized Corrosion of Waste Package Outer Barrier , 2000 .
[8] Omar Suliman Zaroog,et al. Corrosion of Stainless Steels , 1979 .
[9] G. Gdowski. Formulation and make-up of simulate dilute water, low ionic content aqueous solution , 1997 .
[10] R. E. Smallman. Chapter 15 – Oxidation and corrosion , 1985 .