Increasing strength and ductility of magnesium alloy WE43 by equal-channel angular pressing
暂无分享,去创建一个
Y. Estrin | M. Gorshenkov | I. Shchetinin | V. Serebryany | N. Martynenko | S. Dobatkin | G. Raab | E. A. Luk'yanova
[1] J. Kubásek,et al. Exceptional mechanical properties of ultra-fine grain Mg-4Y-3RE alloy processed by ECAP , 2017 .
[2] R. Soltani,et al. The microstructure, texture, and room temperature mechanical properties of friction stir processed Mg-Y-Nd alloy , 2017 .
[3] M. Meyers,et al. Microstructural Evolution and Properties of a Hot Extruded and HPT‐Processed Resorbable Magnesium WE43 Alloy , 2017 .
[4] S. Suwas,et al. Superplasticity in high temperature magnesium alloy WE43 , 2017 .
[5] R. Mishra,et al. A framework for shear driven dissolution of thermally stable particles during friction stir welding and processing , 2016 .
[6] Yufeng Zheng,et al. Study on the in vitro degradation behavior of pure Mg and WE43 in human bile for 60 days for future usage in biliary , 2016 .
[7] Y. Estrin,et al. Strengthening of age-hardenable WE43 magnesium alloy processed by high pressure torsion , 2016 .
[8] Yanyao Jiang,et al. Deformation twinning in hexagonal materials , 2016 .
[9] K. Inal,et al. A review on the effect of rare-earth elements on texture evolution during processing of magnesium alloys , 2016, Journal of Materials Science.
[10] Weiweng Zhang,et al. Superplastic behavior and microstructure evolution of a fine-grained Mg–Y–Nd alloy processed by submerged friction stir processing , 2015 .
[11] Datong Zhang,et al. Microstructure evolution and mechanical properties of Mg–Nd–Y alloy in different friction stir processing conditions , 2015 .
[12] V. Sirotinkin,et al. Structure, texture, and mechanical properties of an MA2-1hp magnesium alloy after two-stage equal-channel angular pressing and intermediate annealing , 2015, Russian Metallurgy (Metally).
[13] Z. Kang,et al. Achieving high strain rate superplasticity in Mg–Y–Nd–Zr alloy processed by homogenization treatment and equal channel angular pressing , 2015 .
[14] D. Choudhuri,et al. Strength and ductility optimization of Mg–Y–Nd–Zr alloy by microstructural design , 2015 .
[15] Zhigang Xu,et al. Recent advances on the development of magnesium alloys for biodegradable implants. , 2014, Acta biomaterialia.
[16] V. Serebryany,et al. Texture and anisotropy of mechanical properties of the magnesium alloy of Mg-Y-Gd-Zr system , 2014, Inorganic Materials: Applied Research.
[17] L. Čížek,et al. Metallographic Analysis of ECAP Processed Selected Magnesium Alloys , 2014 .
[18] H. Okamoto. Supplemental Literature Review of Binary Phase Diagrams: Cs-In, Cs-K, Cs-Rb, Eu-In, Ho-Mn, K-Rb, Li-Mg, Mg-Nd, Mg-Zn, Mn-Sm, O-Sb, and Si-Sr , 2013, Journal of Phase Equilibria and Diffusion.
[19] S. Suwas,et al. Hot Deformation Processing and Texture in Magnesium Alloy WE43 , 2013 .
[20] J. Nie. Precipitation and Hardening in Magnesium Alloys , 2012, Metallurgical and Materials Transactions A.
[21] V. Shkuropatenko,et al. Influence of grain size on mechanical and corrosion properties of magnesium alloy for medical implants , 2009 .
[22] Long-Sen Chang,et al. Improvement of strength of magnesium alloy processed by equal channel angular extrusion , 2008 .
[23] T. Savyolova,et al. ODF Restoration by Orientations Grid , 2005 .
[24] P. Liaw,et al. Texture evolution of five wrought magnesium alloys during route A equal channel angular extrusion: Experiments and simulations , 2005 .
[25] Donald W. Brown,et al. Enhanced ductility in strongly textured magnesium produced by equal channel angular processing , 2004 .
[26] W. Kim,et al. Mechanical properties and microstructures of an AZ61 Mg Alloy produced by equal channel angular pressing , 2002 .