Corrosive effects of salt hydrate phase change materials used with aluminium and copper
暂无分享,去创建一个
[1] R. Jarman,et al. Metal/environment reactions , 1976 .
[2] Luisa F. Cabeza,et al. Immersion corrosion tests on metal‐salt hydrate pairs used for latent heat storage in the 32 to 36°C temperature range , 2001 .
[3] Luisa F. Cabeza,et al. Review on thermal energy storage with phase change: materials, heat transfer analysis and applications , 2003 .
[4] A. V. Turkovskaya,et al. Corrosion and Protection of Metals , 2020 .
[5] F. C. Porisini. Salt hydrates used for latent heat storage: Corrosion of metals and reliability of thermal performance , 1988 .