Enhancement of adhesive joint strength by laser surface modification

This report describes modification of titanium surfaces by means of a laser ablation process that generates microcolumnar arrays (MCA) and thereby increases the adhesive bond strength between titanium plates in many ways. Bond strength improves due to (i) increase in surface area, (ii) mechanical locking of adhesive between microcolumns, and (iii) modifications in the surface chemistry of the adherend and consequent improvement in wettability of adherend/adhesive interface. Due to the enhancement in bond strength, failure of joints moves away from interfaces into the bulk of the adhesive layer, suggesting that the strength-limiting factor is the epoxy strength.

[1]  Catherine A. Ploskonka,et al.  Fundamentals of Composites Manufacturing: Materials, Methods, and Applications , 1989 .

[2]  A. Baldan Adhesively-bonded joints and repairs in metallic alloys, polymers and composite materials: Adhesives, adhesion theories and surface pretreatment , 2004 .

[3]  Tsu-Wei Chou,et al.  Structure and properties of composites , 1993 .

[4]  G. A. Shafeev,et al.  Arrays of 3D micro-columns generated by laser ablation of Ta and steel: modelling of a black body emitter , 2004 .

[5]  J. Comyn,et al.  Corona-discharge treatment of polyetheretherketone (PEEK) for adhesive bonding , 1996 .

[6]  James P. Wightman,et al.  Sodium hydroxide anodization of Ti-Al-4V adherends , 1987 .

[7]  T. M. Young,et al.  Surface treatment of titanium for adhesive bonding to polymer composites: a review , 2001 .

[8]  G. A. Shafeev,et al.  Spectral and surface analysis of heated micro-column arrays fabricated by laser-assisted surface modification , 2004 .

[9]  Chun Huh,et al.  Effects of surface roughness on wetting (theoretical) , 1977 .

[10]  T. M. Yue,et al.  Enhancement of ceramic-to-metal adhesive bonding by excimer laser surface treatment , 1997 .

[11]  J. S. Ahearn,et al.  Adhesion Tensile Testing of Environmentally Exposed Ti-6Al-4V Adherends , 1987 .

[12]  R. Adams Testing of Bonded Joints , 1987 .

[13]  Y. Mai,et al.  Interfaces in Composites , 2006 .

[14]  J. Cotter,et al.  Development of new surface pretreatments, based on alkaline hydrogen peroxide solutions, for adhesive bonding of titanium , 1982 .

[15]  K. L. Mittal,et al.  Adhesive Joints: Formation, Characteristics and Testing , 2023 .

[16]  A. Beevers,et al.  The effects of grit-blasting on surface properties for adhesion , 1999 .

[17]  D. Bond,et al.  Principles and practices of adhesive bonded structural joints and repairs , 1999 .

[18]  P. K. Trojan,et al.  Engineering materials and their applications , 1975 .

[19]  F. Yost,et al.  Extensive wetting due to roughness , 1995 .

[20]  T. M. Young,et al.  Adhesives bonding of a titanium alloy to a glass fibre reinforced composite material , 2002 .

[21]  S. Hashim,et al.  Effect of surface roughness on the strength of cleavage joints , 2002 .