Photochemical Degradation Study of Polyurethanes as Relic Protection Materials by FTIR-ATR

Polyurethanes are one kind of relic protection materials commonly used. During artificial photo-ageing, three polyurethanes, HDI-based polyurethane, MDI-based polyurethane and TDI-based polyurethane, have been considered to undergo UV radiation. Photochemical degradation of the polyurethanes has been monitored by means of Fourier transform infrared spectroscopy with attenuated total reflection accessory (FTIR-ATR). It was proved that the mechanism of the photochemical degradation of polyurethanes might be the scissions of carbamate (urethane) groups and the re-reactions of radical groups formed in the scission reactions. From the experiment results HDI-based polyurethane, an aliphatic diisocyanate, could be considered to be more suitably used as relic protection materials among these three polyurethanes for its ageing products with less color.

[1]  D. Dattelbaum,et al.  Pressure-dependent Fourier transform infrared spectroscopy of a poly (ester urethane). , 2003, Spectrochimica acta. Part A, Molecular and biomolecular spectroscopy.

[2]  D. Tallman,et al.  Degradation of low gloss polyurethane aircraft coatings under UV and prohesion alternating exposures , 2003 .

[3]  R. Sanderson,et al.  Thermogravimetric study of phosphated polyurethane ionomers , 2002 .

[4]  S. Gogolewski,et al.  In vitro degradation of novel medical biodegradable aliphatic polyurethanes based on ϵ-caprolactone and Pluronics® with various hydrophilicities , 2002 .

[5]  B. Legendre,et al.  Degradation of segmented poly(etherurethane) Tecoflex® induced by electron beam irradiation: Characterization and evaluation , 2001 .

[6]  J. Araña,et al.  Highly concentrated phenolic wastewater treatment by the photo-Fenton reaction, mechanism study by FTIR-ATR. , 2001, Chemosphere.

[7]  Y. Grohens,et al.  Electron irradiation of polyesterurethane: study of chemical and structural modifications using FTIR, UV spectroscopy and GPC , 2001 .

[8]  Gordon P. Bierwagen,et al.  Weathering degradation of a polyurethane coating , 2001 .

[9]  E. B. Orler,et al.  Infrared linear dichroism study of a hydrolytically degraded poly(ester urethane) , 2001 .

[10]  E. Duverger,et al.  Electron irradiation of polyurethane: Some FTIR results and a comparison with a EGS4 simulation , 2000 .

[11]  J. Gimeno-Adelantado,et al.  Study by FT-IR spectroscopy of ageing of adhesives used in restoration of archaeological glass objects , 1999 .

[12]  L. Irusta,et al.  Photooxidative behaviour of segmented aliphatic polyurethanes , 1999 .

[13]  M. Chew,et al.  Applicability of infrared spectroscopy for sealant degradation studies , 1998 .

[14]  A. Brandwood,et al.  In-vivo degradation of polyurethanes: transmission-FTIR microscopic characterization of polyurethanes sectioned by cryomicrotomy. , 1997, Biomaterials.