Degradation of poly(lactic-co-glycolic acid) microspheres: effect of copolymer composition.

The in vitro degradation behaviour of a wide range of poly(D,L-lactic-co-glycolic acid) (PLGA) has been examined in terms of degree of degradation and morphological change during an incubation period of up to 53 d. Gel permeation chromatography and differential scanning calorimetry were employed to characterize their degradation profiles. It was found that amorphous PLGA exhibited a transient multiple crystallization behaviour of D- or L-lactic acid oligomers during degradation. This indicated that the hydrolytic scission of ester bonds tends to primarily target the linkage between glycolic acid and D- or L-lactic acid or glycolic acid. In addition, two distinctive glass transition temperatures appeared when these crystallization phenomena occurred, suggesting the transient presence of fast and slowly eroding polymer domains within microspheres during the degradation. This study supports the heterogeneous bulk degradation for PLGA microspheres which has been proposed recently for a large specimen.

[1]  M. Sisido,et al.  Vibrational circular dichroism of polypeptides. 11. Conformation of poly(L-Z-lysine-L-Z-lysine-L-1-pyrenylalanine) and poly(L-Z-lysine-L-Z-lysine-L-1-naphthylalanine) in solution , 1987 .

[2]  Michel Vert,et al.  In vivo degradation of massive poly(α-hydroxy acids): Validation of In vitro findings , 1992 .

[3]  Michel Vert,et al.  Morphological changes resulting from the hydrolytic degradation of stereocopolymers derived from L- and DL-lactides , 1994 .

[4]  Ross R. Muth,et al.  Biodegradable polymers for use in surgery—polyglycolic/poly(actic acid) homo- and copolymers: 1 , 1979 .

[5]  R. Langer,et al.  Biodegradable polymers as drug delivery systems , 1990 .

[6]  D. Crommelin,et al.  Controlled release of bioactive agents from lactide/glycolide polymers , 1990 .

[7]  A. M. Reed,et al.  Biodegradable polymers for use in surgery — poly(glycolic)/poly(Iactic acid) homo and copolymers: 2. In vitro degradation , 1981 .

[8]  D. V. Krevelen Properties of Polymers , 1990 .

[9]  Tae Gwan Park,et al.  Importance of in vitro experimental conditions on protein release kinetics, stability and polymer degradation in protein encapsulated poly (d,l-lactic acid-co-glycolic acid) microspheres , 1995 .

[10]  A. Pennings,et al.  Crystal structure, conformation and morphology of solution-spun poly(L-lactide) fibers , 1990 .

[11]  Tae Gwan Park,et al.  Degradation of poly(d,l-lactic acid) microspheres: effect of molecular weight , 1994 .

[12]  H. V. Maulding Prolonged delivery of peptides by microcapsules , 1987 .

[13]  D. Lewis,et al.  Controlled release of a luteinizing hormone-releasing hormone analogue from poly(d,l-lactide-co-glycolide) microspheres. , 1984, Journal of pharmaceutical sciences.

[14]  B.J.A. Furra,et al.  A biodegradable delivery system for peptides: preclinical experience with the gonadotrophin-releasing hormone agonist Zoladex☆ , 1992 .

[15]  Yoshito Ikada,et al.  Stereocomplex formation between enantiomeric poly(lactides) , 1987 .

[16]  Yoshito Ikada,et al.  Thermal characterization of polylactides , 1988 .

[17]  Michel Vert,et al.  Structure-property relationships in the case of the degradation of massive aliphatic poly-(α-hydroxy acids) in aqueous media , 1990 .

[18]  R. Kenley,et al.  Poly(lactide-co-glycolide) decomposition kinetics in vivo and in vitro , 1987 .

[19]  Michel Vert,et al.  STRUCTURE – PROPERTY RELATIONSHIP IN THE CASE OF THE DEGRADATION OF MASSIVE ALIPHATIC POLY – (-HYDROXY ACIDS) IN AQUEOUS MEDIA, PART 1: DEGRADATION OF LACTIDE - GLYCOLIDE COPOLYMERS: PLA 37.5 GA 25 AND PLA 75 GA 25 , 1990 .

[20]  T. Kondo,et al.  Mechanism of hydrolytic degradation of poly(L-lactide) microcapsules: effects of pH, ionic strength and buffer concentration. , 1986, Journal of microencapsulation.