Data are presented on the acute toxicity (mortality only) of the thermal degradation products of polymers obtained by two methods of degradation. One system utilized a slowly increasing temperature (5 degrees C/min) and gradual degradation of the polymer with the rats being exposed to degradation products as they were evolved. In this system the more toxic polymers included wool, polypropylene, poly(vinyl chloride), and urethane foam. The second system utilized conditions of rapid combustion and exposure of rats to the total products of combustion for a period of 4 hr. In this system the more toxic materials included red oak, cotton, acrylonitrile-butadiene-styrene (ABS), and styrene-acrylonitrile. It is of interest to note that the natural product wool is among the least toxic under these rapid combustion conditions and among the most toxic under slow pyrolysis conditions. Other materials also vary in the comparative toxicity of their thermal degradation products, depending upon the conditions of degradation and animal exposure. The two experimental techniques presented here may well represent the two extreme conditions of rapid combustion versus slow pyrolysis. Intermediate types of fire situations might be expected to result in relative acute toxicities somewhere between these two extremes. This report deals with acute toxicity on the basis of mortality data only and does not include other parameters of toxicity such as organ weights and histopathology.
[1]
H. Cornish,et al.
Toxicity of pyrolysis products of vinyl plastics.
,
1969,
Archives of environmental health.
[2]
J. Zapp.
Toxic and health effects of plastics and resins.
,
1962,
Archives of environmental health.
[3]
An analytical system for identifying the volatile pyrolysis products of plastics.
,
1967,
American Industrial Hygiene Association journal.
[4]
Macfarland Hn,et al.
Hazards From Thermodecomposition of Epoxy Resins
,
1963
.
[5]
K. Leong,et al.
HAZARDS FROM THERMODECOMPOSITION OF EPOXY RESINS.
,
1963,
Archives of environmental health.