Microstructure-fracture behavior correlation of toughened SiCf/SiC composites prepared by vacuum infiltration and hot pressing

[1]  D. Yoon,et al.  Microstructure-flexural strength correlation and efficacy of rare earth nitrates on the sintering of SiCf/SiC composites , 2016 .

[2]  Ji-Yeon Park,et al.  Fabrication of the tube-shaped SiCf/SiC by hot pressing , 2015 .

[3]  B. Min,et al.  Highly dense and fine-grained SiC with a Sc-nitrate sintering additive , 2014 .

[4]  A. Noviyanto,et al.  Rare-earth nitrate additives for the sintering of silicon carbide , 2013 .

[5]  A. Noviyanto,et al.  Metal oxide additives for the sintering of silicon carbide: Reactivity and densification , 2013 .

[6]  D. Yoon,et al.  Properties of SiCf/SiC composites fabricated by slurry infiltration and hot pressing , 2011 .

[7]  Jong-Hyun Lee,et al.  Improvement of SiCf/SiC density by slurry infiltration and tape stacking , 2009 .

[8]  Akira Kohyama,et al.  Current status and critical issues for development of SiC composites for fusion applications , 2007 .

[9]  Z. Haitao,et al.  Application of Rare Earths in Advanced Ceramic Materials , 2007 .

[10]  T. Nishimura,et al.  High-temperature strength of silicon carbide ceramics sintered with rare-earth oxide and aluminum nitride , 2007 .

[11]  S. Dong,et al.  Preparation of C/SiC Composites by Hot Pressing, Using Different C Fiber Content as Reinforcement , 2006 .

[12]  Doh-Yeon Kim,et al.  Grain boundary crystallization during furnace cooling of α-SiC sintered with Y2O3–Al2O3–CaO , 2006 .

[13]  S. Jitsukawa,et al.  Effect of thick SiC interphase layers on microstructure, mechanical and thermal properties of reaction-bonded SiC/SiC composites , 2005 .

[14]  M. Pavese,et al.  Potential of SiC multilayer ceramics for high temperature applications in oxidising environment , 2005 .

[15]  Young‐Wook Kim,et al.  Fine‐Grained Silicon Carbide Ceramics with Oxynitride Glass , 2004 .

[16]  F. Castro,et al.  Liquid phase sintering of SiC with additions of Y2O3, Al2O3 and SiO2 , 2004 .

[17]  F. Aldinger,et al.  Improved high temperature properties of SiC-ceramics sintered with Lu2O3-containing additives , 2003 .

[18]  P. Fino,et al.  High temperature oxidation of multilayered SiC processed by tape casting and sintering , 2002 .

[19]  Mitsutane Fujita,et al.  Effect of nuclear data and impurities on the evaluation of induced activity of CVI SiCf/SiC composites , 2002 .

[20]  A. Kohyama,et al.  Hi-NicalonTM Fiber-Reinforced CVI-SiC Matrix Composites: I Effects of PyC and PyC-SiC Multilayers on the Fracture Behaviors and Flexural Properties , 2002 .

[21]  T. Yano,et al.  Improvement of the mechanical properties of hot-pressed silicon-carbide-fiber-reinforced silicon carbide composites by polycarbosilane impregnation , 2001 .

[22]  Young‐Wook Kim,et al.  Effect of sintering-additive composition on fracture toughness of liquid-phase-sintered SiC ceramics , 2001 .

[23]  N. Igawa,et al.  Mechanical and thermal properties of 2D and 3D SiC/SiC composites , 2000 .

[24]  D. Thompson,et al.  The Use of MgO as a densification aid for α-SiC , 1999 .

[25]  T. Yano,et al.  Fabrication of silicon carbide fiber-reinforced silicon carbide composite by hot-pressing , 1998 .

[26]  W. Clegg,et al.  The fabrication and failure of laminar ceramic composites , 1992 .

[27]  J. Brennan Interfacial studies of chemical-vapor-infiltrated ceramic matrix composites , 1990 .

[28]  C. Kim,et al.  Toughening Behavior of Silicon Carbide with Additions of Yttria and Alumina , 1990 .

[29]  Y. Takeda Development of high-thermal-conductive SiC ceramics , 1988 .

[30]  S. Dapkunas Ceramic heat exchangers , 1988 .

[31]  T. Yano,et al.  Hot-Pressing of β-SiC Powder with Al-B-C Additives , 1986 .