Effects of Au/Ni coating thickness on enhancing the properties of InPb/MoCu solder joints in microwave modules
暂无分享,去创建一个
Jiu-hua Xu | Yucan Fu | W. Ding | Mingyue Xiong | Lei Sun | H. Su | B. Zhao | Zhenghu Zhu | Fan Pu
[1] K. Tu,et al. Low temperature interfacial reaction in 3D IC nanoscale materials , 2022, Materials Science and Engineering: R: Reports.
[2] P. Vianco,et al. Impact of Gold Thickness on Interfacial Evolution and Subsequent Embrittlement of Tin–Lead Solder Joints , 2022, Journal of Electronic Materials.
[3] Y. Lei,et al. Low temperature brazing between pre-metallized ZrO2 ceramics and medical pure titanium using AuSn20 filler metal , 2022, Vacuum.
[4] L. Zhang,et al. Transient liquid phase bonding (TLPB) of Cu to Cu using Sn interconnect solder reinforced by submicron Al particles , 2022, Journal of Materials Processing Technology.
[5] Caiju Li,et al. Revealing effects of common nonmetallic impurities on the stability and strength of Cu–Sn solder joints: A first-principles investigation , 2022, Vacuum.
[6] Qian Sun,et al. Influence mechanism of Au layer thickness on wettability of Sn–Ag–Cu solder on heated ENIG pads , 2022, Vacuum.
[7] Haoran Ma,et al. Effect of substrate surface roughness on interfacial reaction at Sn-3.0Ag/(001)Cu interface , 2022, Vacuum.
[8] R. Kainuma,et al. Formation and growth behavior of intermetallic compound phases in the interfacial reaction of solid Fe / liquid Zn at 450 °C , 2021 .
[9] N. Zhao,et al. Quasi-in-situ observation on diffusion anisotropy dominated asymmetrical growth of Cu-Sn IMCs under temperature gradient , 2021 .
[10] Wenchao Yang,et al. Interfacial reaction and mechanical properties of Sn58Bi-XCr solder joints under isothermal aging conditions , 2021, Vacuum.
[11] Liang Zhang,et al. Interfacial reaction, shear behavior and microhardness of Cu-Sn TLP bonding joints bearing CuZnAl powder for 3D packaging , 2021, Journal of Manufacturing Processes.
[12] E. Novitskaya,et al. Hall–Petch effect in binary and ternary alumina / zirconia / spinel composites , 2021 .
[13] Yanhong Tian,et al. Comparative study between the Sn–Ag–Cu/ENIG and Sn–Ag–Cu/ENEPIG solder joints under extreme temperature thermal shock , 2021, Journal of Materials Science: Materials in Electronics.
[14] S. Jung,et al. Effect of Ni(P) thickness in Au/Pd/Ni(P) surface finish on the electrical reliability of Sn–3.0Ag–0.5Cu solder joints during current-stressing , 2021 .
[15] L. Zhang,et al. Materials modification of the lead-free solders incorporated with micro/nano-sized particles: A review , 2021 .
[16] Zheng-qiu Wu,et al. Growth of the nano-phase intermetallic compounds and its effect on mechanical behavior of Au80Sn20/CrMnFeCoNi solder joints during isothermal aging , 2020 .
[17] O. Oloyede,et al. Tensile, hardness and microstructural properties of Sn-Pb solder alloys , 2020 .
[18] Xiaowu Hu,et al. Shear strength and fracture surface analysis of lead-free solder joints with high fraction of IMCs , 2020 .
[19] Xiaowu Hu,et al. Effect of Co addition into Ni film on shear strength of solder/Ni/Cu system: Experimental and theoretical investigations , 2020 .
[20] Hailong Li,et al. Effect of nickel metallization thickness on microstructure evolution and mechanical properties in Sn3.0Ag0.5Cu/Au/Ni/Cu solder joints , 2020, Journal of Materials Science: Materials in Electronics.
[21] K. Tu,et al. A high-entropy alloy as very low melting point solder for advanced electronic packaging , 2020, 2006.01345.
[22] Xiaowu Hu,et al. Effects of Ni modified MWCNTs on the microstructural evolution and shear strength of Sn-3.0Ag-0.5Cu composite solder joints , 2020 .
[23] S. Jung,et al. Effects of crystalline and amorphous Pd layers on initial interfacial reactions at Sn-3.0Ag-0.5Cu/thin-Au/Pd/Ni(P) solder joints , 2020 .
[24] Liang Zhang,et al. Inhibition of intermetallic compounds growth at Sn–58Bi/Cu interface bearing CuZnAl memory particles (2–6 μm) , 2020, Journal of Materials Science: Materials in Electronics.
[25] S. Jung,et al. Optimal Ni(P) thickness and reliability evaluation of thin-Au/Pd(P)/Ni(P) surface-finish with Sn-3.0Ag-0.5Cu solder joints , 2019, Journal of Alloys and Compounds.
[26] P. He,et al. Effect of CuZnAl particles addition on microstructure of Cu/Sn58Bi/Cu TLP bonding solder joints , 2019, Vacuum.
[27] Xiaowu Hu,et al. Insights on interfacial IMCs growth and mechanical strength of asymmetrical Cu/SAC305/Cu-Co system , 2019, Vacuum.
[28] Liang Zhang,et al. Stress analysis and structural optimization of 3-D IC package based on the Taguchi method , 2019, Soldering & Surface Mount Technology.
[29] Xiaowu Hu,et al. Effect of Cu additions on mechanical properties of Ni3Sn4-based intermetallic compounds: First-principles calculations and nano-indentation measurements , 2019, Vacuum.
[30] Liang Zhang,et al. Microstructure evolution and grain orientation of IMC in Cu-Sn TLP bonding solder joints , 2019, Journal of Alloys and Compounds.
[31] K. Tu,et al. Recent advances on kinetic analysis of solder joint reactions in 3D IC packaging technology , 2019, Materials Science and Engineering: R: Reports.
[32] Yulong Li,et al. Influences of Mono-Ni(P) and Dual-Cu/Ni(P) Plating on the Interfacial Microstructure Evolution of Solder Joints , 2018, Metallurgical and Materials Transactions A.
[33] Liang Zhang,et al. Interface reaction and intermetallic compound growth behavior of Sn-Ag-Cu lead-free solder joints on different substrates in electronic packaging , 2018, Journal of Materials Science.
[34] Chih-Ming Chen,et al. Suppression effect of Ni grain size on the Ni3Sn4 growth at the Sn/Ni interface , 2017 .
[35] Tao Xu,et al. Shear strength and fracture behavior of reflowed Sn3.0Ag0.5Cu/Cu solder joints under various strain rates , 2017 .
[36] L. Keer,et al. Microstructure evolution and shear fracture behavior of aged Sn3Ag0.5Cu/Cu solder joints , 2016 .
[37] T. Langdon,et al. Structural impact on the Hall–Petch relationship in an Al–5Mg alloy processed by high-pressure torsion , 2015 .
[38] C. E. Ho,et al. Pronounced effects of Ni(P) thickness on the interfacial reaction and high impact resistance of the solder/Au/Pd(P)/Ni(P)/Cu reactive system , 2014 .
[39] M. Rappaz,et al. Growth of intermetallic compounds in the Au-In system: Experimental study and 1-D modelling , 2014 .
[40] S. Xue,et al. Interface reaction between SnAgCu/SnAgCuCe solders and Cu substrate subjected to thermal cycling and isothermal aging , 2012 .
[41] Jungil Park,et al. Formation and behavior of Kirkendall voids within intermetallic layers of solder joints , 2011 .
[42] P. Vianco,et al. Interface reactions between 50In–50Pb solder and electroplated Au layers , 2005 .
[43] T. Chuang,et al. Interfacial reactions between liquid indium and Au-deposited substrates , 2000 .
[44] H. Okamoto. In-Ni (Indium-Nickel) , 1999 .