Influence of Carding Technique on Yarn Tenacity Response to Increasing Rotor Speed

2. Byme, K. M., Roberts, M. W., and Ross, J. R. H., The Critical Surface Tension of Wool, Textile Res. J. 49, 34-40, (1979). 3. Earle, R. H., Saunders, R. H., and Kangas, L. R., The Chemistry of the Chlorination/Hercosett Resin Shrinkproofing Process, Appl. Polym. Symp. 18, 707-714 (1971). 4. Feldtman, H. D., and McPhee, J. R., The Spreading and Adhesion of Polymers on Wool, Textile Res. J. 34, 634 (1964). 5. Feldtman, H. D., McPhee, J. R., and Morgan, W. V., Shrinkproofing Wool Tops, Textile Manuf. 93, 122124 (1967). 6. Tester, D. H. and Makinson, K. R., A TEM Study of the Causes of Failure in the Chlofine-Hercosett ShrinkResist Process, Textile Res. J. 53, 415-419 (1983). 7. Watt, I. C., Hafey, M. J., and Capablanca, J. S., The Uniformity of Surface Treatments to Wool Fibers, J. Appl. Polym. Sci. (in preparation).