Cyclic Deformation of Rare-Earth Containing Magnesium Alloys

Cyclic deformation characteristics of a rare-earth (RE) element containing extruded Mg-10Gd-3Y-0.5Zr (GW103K) magnesium alloy were evaluated via strain-controlled low-cycle fatigue tests under varying strain amplitudes. Microstructural observations revealed that this alloy consisted of fine equiaxed grains and a large number of RE-containing precipitates. Unlike the RE-free extruded magnesium alloys, this alloy exhibited essentially cyclic stabilization and symmetrical hysteresis loop due to relatively weak crystallographic textures and reduced twinning-detwinning activities. The fatigue life of the present alloy was observed to be longer than that of the RE-free extruded magnesium alloys, which could also be described by the Coffin-Manson law and Basquins equation. Fatigue crack was observed to initiate from the specimen surface and crack propagation was basically characterized by fatigue striations.

[1]  Guohua Wu,et al.  Grain refinement and fatigue strengthening mechanisms in as-extruded Mg–6Zn–0.5Zr and Mg–10Gd–3Y–0.5Zr magnesium alloys by shot peening , 2013 .

[2]  J. Hirsch,et al.  Superior light metals by texture engineering: Optimized aluminum and magnesium alloys for automotive applications , 2013 .

[3]  W. Ding,et al.  Cyclic deformation and fatigue of extruded Mg–Gd–Y magnesium alloy , 2013 .

[4]  Zhen-hua Chen,et al.  The cyclic softening and evolution of microstructures for Mg–10Gd–2.0Y–0.46Zr alloy under low cycle fatigue at 573 K , 2012 .

[5]  J. Murray,et al.  Climate policy: Oil's tipping point has passed , 2012, Nature.

[6]  A. Luo,et al.  Effect of twinning, slip, and inclusions on the fatigue anisotropy of extrusion-textured AZ61 magnesium alloy , 2011 .

[7]  Qudong Wang,et al.  Enhanced very high cycle fatigue performance of extruded Mg-12Gd-3Y-0.5Zr magnesium alloy , 2011 .

[8]  T. Pollock Weight Loss with Magnesium Alloys , 2010, Science.

[9]  A. Luo,et al.  Effect of strain ratio and strain rate on low cycle fatigue behavior of AZ31 wrought magnesium alloy , 2009 .

[10]  A. Luo,et al.  Low cycle fatigue properties of an extruded AZ31 magnesium alloy , 2009 .

[11]  A. Luo,et al.  Strain-Controlled Low-Cycle Fatigue Properties of a Newly Developed Extruded Magnesium Alloy , 2008 .

[12]  Yi Fang,et al.  High Cycle Fatigue Properties of Die-Cast Magnesium Alloy AZ91D with Addition of Different Concentrations of Cerium , 2006 .

[13]  Zhike Peng,et al.  Grain refining mechanism in Mg–9Gd–4Y alloys by zirconium , 2005 .

[14]  K. Kainer,et al.  Magnesium alloys and technology , 2003 .

[15]  S. Suresh Fatigue of materials , 1991 .